Chase Corporation
Chase Corporation Protective Coatings and Electronic Materials
Chase Corporation manufactures protective materials, adhesives, sealants, coatings, and specialty chemicals for electronics, infrastructure, industrial, aerospace, and energy applications. The portfolio includes conformal coatings, surface-treatment and cleaning materials, thinners, encapsulants, underfills, and adhesives used where environmental protection, assembly reliability, and controlled processing are important.
As an authorized Chase Corporation distributor, Krayden supplies selected Humiseal™ and AB Chimie™ materials and provides technical guidance for product selection, substrates, application requirements, and manufacturing processes. Product-specific compatibility, application method, cure behavior, and processing requirements should be confirmed for the exact material selected.
Markets Served by Chase Corporation
Featured Chase Corporation Brands
Explore Chase Corporation brands represented in the source portfolio for conformal coatings, cleaning materials, surface preparation, thinners, and protective electronic materials.

Humiseal™
Conformal coatings and protective materials for electronic assemblies exposed to moisture, contaminants, chemicals, and other demanding operating conditions.

AB Chimie™
Conformal coatings, cleaning and defluxing materials, thinners, and related protective materials for printed circuit board and electronics manufacturing processes.
Conformal Coatings
Chase Corporation conformal-coating materials represented in the source include polyurethane, acrylic, acrylate, and synthetic-rubber technologies for protecting electronic assemblies. Selection depends on the coating chemistry, application and cure process, required environmental protection, and the service conditions of the finished assembly.
Surface Treatments and Thinners
The source portfolio includes cleaning and defluxing materials used in surface preparation together with specialty thinners used to adjust coating application characteristics or support process cleaning. Selection depends on the material being applied or removed, substrate compatibility, required evaporation or application behavior, and the production process.
Encapsulants & Underfills
Encapsulants and underfills protect electronic components and assemblies from environmental exposure and mechanical or thermal stresses. Material selection should consider flow behavior, fill geometry, cure process, optical requirements where applicable, substrate compatibility, and the expected operating environment.
Adhesives
The Chase Corporation source portfolio includes adhesive materials for industrial and electronic assembly, including UV-curable systems for precision bonding. Selection should account for substrate compatibility, joint geometry, cure access, dispensing method, production speed, and the environmental and mechanical requirements of the finished assembly.
Talk to our Experts
Whether you need help comparing conformal coatings, evaluating surface-treatment or thinner options, selecting an encapsulant or adhesive, or matching a material to your manufacturing process, Krayden can help review application requirements and product-selection considerations for Chase Corporation materials.
Chase Corporation Quick Reference
135 products
-
ABchimie DVS Silicone Thinner
- Specially formulated for silicone conformal coatings
- Supports spray and dip application
- Maintains viscosity in open-tank dip systems
-
ABchimie LDM High-Temperature Solder Mask
- Dries at room temperature
- Withstands temperatures up to 270°C
- Can be completely removed by hand
-
ABchimie DVU Urethane Thinner
- Formulated for urethane‑based conformal coatings
- For dip coating and spray coating applications
- Consistent, stable solvent composition
-
-
ABchimie DVP Permanent Coating Stripper
- Designed for controlled application
- Strong solvency
- Easy to apply and remove
-
ABchimie APS AC31 Acrylic Thinner
- Formulated for acrylic conformal coatings
- Provides stable evaporation behavior
- Enables viscosity control
-
Humiseal Thinner 521EU
- RoHS Directive 2002/95/EC compliant
- For use with HumiSeal conformal coatings
- Ensures proper viscosity adjustment
-
ABchimie DVA BA Non-Toxic Acrylic Thinner
- Non‑toxic solvent blend
- For AVR80 BA acrylic coating
- Easy to mix
-
ABchimie DVA XY Acrylic Thinner
- Designed for acrylic conformal coatings
- Optimized for AVR80 XY
- Ensures proper viscosity for dip, spray, and automated coating processes
-
HumiSeal Thinner 64
- RoHS Directive 2015/863/EU compliant
- Ensures proper viscosity adjustment
- For use with HumiSeal 2A64
-
HumiSeal Thinner 73
- RoHS Directive 2015/863/EU compliant
- Ensures proper viscosity adjustment
- For use with 1B73 and 1A20
-
HumiSeal Thinner 503
- RoHS Directive 2015/863/EU compliant
- Ensures proper viscosity adjustment
- Compatible with HumiSeal 1B12, 1B31, 1B66, and 1B73
-
HumiSeal Thinner 505
- RoHS Directive 2015/863/EU compliant
- Ensures proper viscosity adjustment
- Compatible with HumiSeal 1R32 and 1R32A-2
-
HumiSeal Thinner 521
- RoHS Directive 2015/863/EU compliant
- Ensures proper viscosity adjustment
- Compatible with multiple HumiSeal conformal coatings
-
HumiSeal Thinner 600
- RoHS Directive 2011/65/EC compliant
- Compatible with multiple HumiSeal conformal coatings
- Specialty thinner
-
HumiSeal Thinner 602-245
- RoHS Directive 2011/65/EU compliant
- For acrylic conformal coatings
- Ensures proper viscosity adjustment
-
HumiSeal Thinner 604
- RoHS Directive 2011/65/EC compliant
- Specialty thinner
- For use with 1B31EPA and 1B73EPA
-
HumiSeal Thinner 673
- RoHS Directive 2015/863/EU compliant
- For use with acrylic conformal coatings
- Ensures proper viscosity adjustment
-
HumiSeal Thinner 701
- RoHS Directive 2011/65/EC compliant
- For use with multiple HumiSeal conformal coatings
- Ensures proper viscosity adjustment
-
-
-
-
-
-
-
HumiSeal Thinner 535
- RoHS Directive 2015/863/EU compliant
- Ensures proper viscosity adjustment
- Compatible with 2A53 conformal coating
-
HumiSeal Stripper 1063
- Non-Acidic Polyurethane Removal
- Controlled One-Hour Soak
- Clear Low-Density Stripper
-
-
RESIN DESIGNS EMI-CSI-M3
- Combined EMI Shielding and Sealing
- No-Mix Precured Rope Installation
- -40 to 150 deg C Operation
-
-
-
ABchimie R3231 1-Part Neutral Cure Sealant
- Meets MIL-A-46146B requirements
- UL94 V-1 compliant
- Non-corrosive, neutral alkoxy cure
-
ABchimie ABclean Cleaning & Defluxing Solvent
- Fast‑drying, non‑toxic cleaning solvent
- Leaves no greasy or sticky residues after evaporation
- High compatibility with a wide range of plastic materials
-
-
ABchimie ABMousse Hyperactive Foam
- Suitable for plastics, metals, and glass
- CFC‑free formulation
- Effectively removes static charges
-
-
-
ABchimie CIPEX40 Aqueous Base for PCB Cleaners
- Ready‑to‑use aqueous formulation
- Low‑foaming chemistry
- High cleaning efficiency
-
ABchimie CIPEX50 Aqueous Base for PCB Cleaners
- Highly concentrated aqueous cleaning formulation
- Low‑foaming formula
- High cleaning efficiency
-
ABchimie Cipex52 Water-Based PCB cleaner
- Low‑foaming formula
- Strong material compatibility with plastics and metals
- Adjustable concentration
-
ABchimie DET Cleaning and Defluxing Solvent
- Allows easy peeling without scratching surfaces
- 100% ozone-friendly, non-halogenated formula
- Available in aerosol and bulk packaging
-
ABchimie DRP10-2 Silicone Residue Cleaner
- Powerful solvent action for rapid cleaning
- Removes grease, flux, silicone residues, and general dirt
- Low toxicity compared to conventional halogenated solvents
-
ABchimie ISO Cleaner
- Fast-drying, non-toxic solvent formulation
- Excellent compatibility with plastics and elastomers
- Efficiently removes greases, oils, and flux residues from PCBs
-
ABchimie MADEX 250 Cured Coating Cleaner
- Highly effective at removing uncured and cured conformal coatings
- Suitable for cleaning metal and plastic tools, equipment, and frames
- Concentrated formula
-
ABchimie NCC Cleaner
- Fast-drying solvent system
- Compatible with most plastics and surface coatings
- Removes solder paste and uncured adhesives effectively
-
ABchimie NCE Fast-Drying Solvent
- Leaves surfaces perfectly clean and dry
- Fast-drying solvent for efficient cleaning
- Harmless to most plastics, rubbers, elastomers, and coatings
-
ABchimie NDD Cleaner, Degreaser & Flux Remover
- Fast-drying
- 100% ozone-friendly
- Broad material compatibility
-
ABchimie 80K UV High Viscosity Resin
- Soft, shock‑absorbing resin
- Excellent adhesion
- One‑component formulation
-
ABchimie 80K UV LED High Viscosity Resin
- Soft, flexible resin
- Excellent adhesion
- UL 94 V‑0 flammability rating
-
HumiSeal AR10 Low Outgas Acrylic Conformal Coating
- Low Outgassing Conformal Coating
- Fluorescent for Inspection
- Ideal for Aerospace Applications
-
-
HUMISEAL 1A33/521PB65 URETHANE CONFORMAL COATING
- 67.5 +/- 2.5 cP Preblend
- Printed-Circuit-Assembly Moisture Protection
- IPC, MIL, and UL Compliance
-
Humiseal 1B51NSLU D40 | Synthetic Rubber Conformal Coating
- 10-Minute Handling-Dry Coating
- Below 1 g/m^2 day mil MVTR
- Flexible UV-Fluorescent Reworkable Coating
-
HUMISEAL 1A33/521PB25
- Ready for Automated Spray Processing
- Environmental Protection with Inspectability
- UL 94 V-0 Classification
-
HUMISEAL 1B31/521 Acrylic Conformal Coating
- 65 +/- 5 cP Preblend
- Fast-Drying Moisture Protection
- Strong Cured Electrical Properties
-
HUMISEAL 1B73/521
- Ready for Automated Spray Processing
- 30-Minute Handling Time
- 50-Cycle -65 to 125 deg C Thermal Shock
-
HUMISEAL 1B31-S
- Rapid Acrylic Film Handling
- UV-Assisted Coating Inspection
- Ambient or Accelerated Cure
-
HUMISEAL 1B51NS-60
- Low Moisture-Vapor Transmission
- Rapid Synthetic-Rubber Handling
- Flexible Low-Stress Protection
-
HUMISEAL 1B51NSLU/521EU
- 521EU Thinner Compatibility
- Low-Permeability Flexible Film
- Room-Temperature and Heat Cure
-
HUMISEAL 1R32A-2/505
- Ten-Minute Handling Dry
- Ready-to-Use Acrylic Pre-Blend
- UV-Fluorescent Coverage Inspection
-
-
-
HUMISEAL 2A20
- Adhesive and Encapsulant Function
- 10-Minute Handling Time
- Mechanical and Thermal Shock Resistance
-
HUMISEAL 2E10-B
- Extended 60-Minute Pot Life
- Simple 1:1 System Mixing
- High Dielectric Strength Encapsulation
-
-
HUMISEAL 2E42T-B
- Thermally Conductive Electronic Encapsulation
- Extended 60-Minute Pot Life
- Simple 1:1 System Mixing
-
HUMISEAL 2UV11
- UV-Gelled Shadow-Area Encapsulation
- Fast 15-Minute Handling
- Soft Shore A30 Encapsulation
-
HUMISEAL UV12
- Fast 30-Second UV Handling
- Low-Viscosity Optical Encapsulation
- Water-White LED Encapsulation
-
-
-
HUMISEAL UV23LV
- Low-Viscosity Multi-Substrate Bonding
- Fast 30-Second UV Handling
- Dual Secondary Cure Options
-
-
ABchimie 6025UV LED Soft Thixotropic Resin
- One component
- UV LED Cure
- Shock Absorbing
-
-
-
-
ABchimie 6028UV UV LED Cure Thixotropic Resin
- One-component
- Fast UV Curing
- Excellent adhesion to plastics
-
-
-
ABchimie AVR80 BA GEL Removable Acrylic Coating
- Can be soldered through
- Wide temperature range -65°C to +150°C
- Excellent adhesion
-
ABchimie AVR80 BA Non-Toxic Acrylic Coating
- Fluoresces under UV light
- Excellent adhesion
- Halogen‑free formulation
-
ABchimie AVR80 GEL Removable Acrylic Coating
- Excellent adhesion
- Wide temperature range (-65°C to +150°C.)
- Resistant to mold growth.
-
-
ABchimie AVR80 XY Removable Acrylic Coating
- Excellent dielectric properties
- Wide operating temperature range (-65°C to +150°C)
- Removable
-
ABchimie526UV LED Soft Dual Cure Conformal Coating
- One Component
- Dual Cure (UV and Humidity)
- Low Viscosity
-
ABchimie526UV Soft Dual Cure Conformal Coating
- One Component
- Dual Cure (UV and Humidity)
- Low viscosity
-
ABchimie746E UV LED Soft UV Cure Conformal Coating
- Excellent adhesion
- UV‑fluorescent for easy inspection
- Certified UL94 V‑0 and UL746E
-
ABchimie746E UV Soft UV Cure Conformal Coating
- Excellent adhesion
- Fast curing under UV exposure
- Can be soldered through
-
ABchimie800UV LED Soft Dual Cure Conformal Coating
- One Component
- Dual Cure (UV LED and Humidity)
- High Edge Coverage
-
ABchimie800UV Soft Dual Cure Conformal Coating
- One Component
- Dual Cure (UV and Humidity)
- High Edge Coverage
-
-
ABchimie836UV LED Soft Dual Cure Conformal Coating
- One Component
- Dual Cure (UV LED and Humidity)
- Excellent Moisture Resistance
-
ABchimie836UV Soft Dual Cure Conformal Coating
- One Component
- Dual Cure (UV and Humidity)
- Excellent Moisture Resistance
-
Humiseal 1A20 | Fast-Curing Polyurethane Conformal Coating
- Fast-curing
- Fluoresces under UV light
- Flexible and repairable
-
-
-
HumiSeal 1A27LTX Urethane Conformal Coating
- Single-component polyurethane conformal coating
- UL 94 V-0 Flame Retardant
- No free isocyanates
-
-
Humiseal 1A33 | Urethane Conformal Coating
- Urethane Conformal Coating
- Transparent (UV Fluorescent)
- Low moisture vapor permeability
-
Humiseal 1A33 GEL | Thixotropic Polyurethane Paste
- Thixotropic Gel Consistency
- Solvent-Free and No Free Isocyanates
- UV Fluorescence for Inspection
-
HumiSeal 1A33 SEC Urethane Conformal Coating
- Single-component polyurethane conformal coating
- Fluoresces under UV light for inspection
- No free isocyanates
-
HumiSeal 1A33LOS Urethane Conformal Coating
- Fluoresces under UV light for easy inspection
- Low moisture vapor permeability
- No free isocyanates
-
HumiSeal 1A33LTX Urethane Conformal Coating
- Fluoresces under UV light for easy inspection and rework
- Available in pre-blended viscosities for immediate use
- Easy application using automated coating systems
-
HumiSeal 1A33NS Urethane Conformal Coating
- Fluoresces under UV light for inspection
- Low moisture vapor permeability
- Fast drying to handle (15 minutes)
-
-
-
Humiseal 1B15 | Fast-Drying Acrylic Conformal Coating
- One-component
- Superior flexibility and abrasion resistance
- MIL-I-46058C, Type AR Compliant
-
HumiSeal 1B18 Acrylic Conformal Coating
- Single‑component acrylic formulation
- Excellent flexibility
- RoHS compliant & UL recognized
-
-
HumiSeal 1B31 245 Acrylic Conformal Coating
- Single‑component acrylic formulation
- Easily repairable
- MIL‑I‑46058C, AR qualified
-
HumiSeal 1B31 LTX Acrylic Conformal Coating
- Available in multiple pre‑blends
- Reduced xylene and toluene
- Low moisture vapor permeability
-
-
HumiSeal 1B31LOC Acrylic Conformal Coating
- Low VOC formulation
- Strong electrical insulation properties
- MIL‑I‑46058C qualified
-
HumiSeal 1B31S Acrylic Conformal Coating
- MIL‑I‑46058C qualified
- IPC‑CC‑830 compliant
- RoHS compliant (Directive 2002/95/EC)
-
Humiseal 1B51 | Synthetic Rubber Conformal Coating
- One-component
- Superior flexibility and abrasion resistance
- MIL-I-46058C Compliant
-
Humiseal 1B51NS | One-Component Synthetic Rubber Conformal Coating
- Fast-drying formula
- Low moisture vapor permeability
- Flexible & low stress
-
Humiseal 1B51NSLU | Synthetic Rubber Conformal Coating
- Fast-drying
- Low moisture vapor permeability
- Environmentally friendly
-
Humiseal 1B73 | Acrylic conformal coating
- Acrylic Conformal Coating
- Transparent (UV Fluorescent)
- Dielectric Strength - 6300 V
-
HumiSeal 1B73EPA Acrylic Conformal Coating
- RoHS compliant (Directive 2002/95/EC)
- UL recognized (File No. E105698)
- EPA 33/50 & IPC‑CC‑830 compliant
-
-
HumiSeal 1B73LOC Acrylic Conformal Coating
- MIL‑I‑46058C qualified
- RoHS Directive 2011/65/EU compliant
- UL recognized (File Number E105698)
-
Humiseal 1C49 | High Build, VOC-Free Silicone Conformal Coating
- VOC-free
- High build
- Fluoresces under UV light
-
Humiseal 1C49LV | Low-Viscosity Silicone Conformal Coating
- VOC-free
- Fluoresces under UV light
- Compatible for use in aerospace applications
-
Humiseal 1C51 | Low-Viscosity, Fast Thermal Curing Silicone Conformal Coating
- VOC-free
- Fast thermal curing
- Fluoresces under UV light
-
Humiseal 1C53 | Low-Viscosity, Fast Thermal Curing Silicone Conformal Coating
- VOC-free
- Fast thermal curing
- Fluoresces under UV light
-
Humiseal 1C55 | Low-Viscosity, Fast Thermal Curing Silicone Conformal Coating
- VOC-free
- Fast thermal curing
- Low viscosity
-
Humiseal 1C63 | UV/RTV Curing, Oxime-Type Cure Silicone Conformal Coating
- UV/RTV curing
- Non-corrosive
- Excellent weather resistance
-
Humiseal 1R32 | Fast-Drying, One-Component Acrylic Conformal Coating
- One-component
- Fast-drying
- Excellent moisture & environmental protection
-
Humiseal 1R32A-2 | Fast-Drying Acrylic Conformal Coating with Improved Adhesion
- Improved adhesion to typical substrates
- Fast-drying
- Range of Pre-blends available for different application methods
-
Humiseal 2A64 | Urethane Conformal Coating
- Exceptional Electrical Insulation
- Easy Quality Control
- High environmental resistance
-
-
Humiseal UV20GEL | High Performance Staking and Vibration Protection UV Gel
- Thixotropic Gel Consistency
- Fast UV Cure
- Shadow Area Cure
-
Humiseal UV40 | Acrylated Urethane Conformal Coating
- Acrylated Urethane Conformal Coating
- Secondary cure mechanism cures any unexposed areas
- Excellent chemical and moisture resistance
-
Humiseal UV50LV | Low-Viscosity UV Curable Conformal Coating
- Fast UV cure
- Fluoresces under UV light
- UL Recognized (File Number E105698)
-
Humiseal UV92 | Urethane acrylate UV masking material
- Easily Applied by syringes, dispensing machines
- Keeps contact points and connections free of coating
- Easily removed by peeling - leaves no residue to interfere with subsequent operations