ABchimie AVR80 GEL Removable Acrylic Coating

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ABchimie AVR80 GEL Removable Acrylic Coating

Main features

  • Excellent adhesion
  • Wide temperature range (-65°C to +150°C.)
  • Resistant to mold growth.

Product Description

ABchimie AVR80 GEL is a flexible, transparent acrylic gel coating designed for the protection of electronic circuitry requiring high‑performance environmental resistance. Its gel‑like viscosity allows the formation of dams and high‑thickness deposits, making it ideal for applications where additional mechanical or environmental protection is needed.

The coating is repairable and can be fully removed using ABchimie SND or DNS, both of which are 100% ozone‑friendly. AVR80 GEL combines strong adhesion, excellent dielectric properties, and reliable performance across a wide temperature range, ensuring dependable long‑term protection.

Product Key Features

  • Flexible, transparent acrylic gel coating
  • Allows damming and high‑thickness coating deposits
  • Excellent adhesion in a wide range of climatic conditions
  • Fluoresces under UV light for easy inspection
  • Wide operating temperature range (–65°C to +150°C)

Applications

  • High‑thickness conformal coating for PCBs
  • Damming and gel barrier applications for selective coating areas
Product Family

ABC-AVR80GEL/1LB

Vernis Acrylique Réparable GEL 01L
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Can
Net weight 0.96 kg
Gross weight 1.1 kg
Dimensions 9 x 9 x 21 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent thixotropic liquid with blue reflection
Density (g)
0.96 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
25 °C

Additional Information

Product Selector Guide Between AVR80 BA GEL and AVR80 GEL

Property AVR80 BA GEL AVR80 GEL
Type Flexible, transparent acrylic gel coating Gel‑form acrylic for high‑thickness deposits
Transparency
Transparent gel
Ultra‑clear gel for optical/sensor application
Form / Viscosity Gel consistency Gel consistency
Operating Temperature −65 °C to +150 °C −65 °C to +150 °C
Removability Fully removable with ABchimie SND or ABclean Removable with ABchimie SND or DNS
Solder‑Through Capability Yes, no toxic gases produced Yes, no isocyanates present
Drying / Curing Air‑dries at room temperature Touch‑dry <30 min; full cure 24h
Advantages Applications requiring non‑toxic, thick protective gel layers (dams, barriers) Applications requiring optical clarity, sensor encapsulation, or transparent high‑thickness protection

Instructions for Use

Workshop temperatures of less than 16°C or relative humidities in excess of 75% are unsuitable for the application of AVR80 GEL.

Before coating Pcbs must be clean, dry and without moisture. The CI being humidity sensor, it is important to remove it before coating. A passage in oven from 1 to 2 hours at 60°C is generally enough.

AVR80 GEL contains a UV trace which allows inspection of the PCB after coating to ensure complete and even coverage. The stonger the reflected light, the thicker the coating layer is.

Drying Times and Curing Conditions

AVR80 GEL will be touch dry after few minutes at room temperature and does not require a thermal cure. The full properties of AVR80 will be obtained after a 24 hours at room temperature.

Removing AVR80 GEL

AVR80 GEL can be soldered through. But, if necessary, it can be easily removed with SND or DNS solvents. To remove AVR80 GEL, dip the full PCBA into a bath of SND during 3 to 10 minutes (depending the thickness of the gel). Then, brush it and after that rince the PCB with SND. To remove AVR80 GEL locally, use SND400B (aerosol) and work with absorbent paper to eliminate all the gel.