Humiseal 1B12 | Acrylic Conformal Coating

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Humiseal 1B12 | Acrylic Conformal Coating

Main features

  • One-component
  • Fast-drying
  • Excellent flexibility

Product Description

HumiSeal 1B12 is a single-component, fast-drying acrylic conformal coating. It provides excellent moisture and environmental protection for printed circuit assemblies. This coating is known for its toughness and abrasion resistance. For streamlined inspection, it fluoresces under UV light. It is MIL-I-46058C qualified and adheres to the RoHS Directive 2002/95/EC.

Product Key Features

  • Single-component formula - No mixing required.
  • Fast-drying - Speeds up production time.
  • Excellent flexibility for durable protection.
  • Fluoresces under UV light for easy inspection.

Applications

Product Family

HS-1B12/5LC

5-Liter Can
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 12 weeks
Packaging
Unit of measure Bottle
Net weight 4.45 kg
Gross weight 4.9 kg
Dimensions 16.8 x 10.6 x 32 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.89 g/cm3
Solids
21.5 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
32 °C
Operating Temperature
-65 - 125 °C
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
1500 V

Additional Information

Frequently Asked Questions About HumiSeal® 1B12

What are typical applications for HumiSeal® 1B12?


HumiSeal® 1B12 is a general-purpose, single-component, fast air drying acrylic conformal coating that is used for protecting printed circuit board assemblies (PCBs) in various industries, including:

  • Aerospace systems (e.g., avionics, control modules)
  • Automotive electronics (e.g., engine control units, sensors)
  • Industrial automation (e.g., motor drives, PLCs)
  • Consumer electronics (e.g., smartphones, gaming devices)

Why choose HumiSeal® 1B12 over other conformal coatings?


HumiSeal® 1B12 is easy to use and provides excellent protection. It provides excellent electrical insulation, fluoresces under UV for easy inspection, and is easily repairable with HumiSeal® Stripper 1080. It is also compliant with MIL-I-46058C, and RoHS 2002/95/EC, making it a trusted choice for demanding applications. You can learn how to select a conformal coating in our latest blog.

What is the shelf life of HumiSeal® 1B12?

HumiSeal® 1B12 has a shelf life of 18 months from the date of manufacture when stored at room temperature (0 to 35°C) in tightly closed containers. Prior to use, allow the product to equilibrate for 24 hours at 18 to 32°C to ensure optimal performance.

How should I clean tools after applying HumiSeal® 1B12?

Tools and equipment used for applying HumiSeal® 1B12 (e.g., spray guns, brushes, or dipping tanks) can be cleaned using HumiSeal® Thinner 521 for spraying and Thinner 503 for dipping & brushing. For removing the coating from PCBs during rework, use HumiSeal® Stripper 1080 or 1080A. Always use a lint-free cloth and ensure proper ventilation during cleaning.

What happens to HumiSeal® 1B12 after its shelf life?

Past its 18-month shelf life, HumiSeal® 1B12 may experience changes in viscosity, which could affect application consistency and coating uniformity. Using expired product may lead to suboptimal performance, and the manufacturer will not be liable for quality or performance issues if expired material is used.

Why do curing times vary for HumiSeal® 1B12?

HumiSeal® 1B12 is a fast air drying coating. Drying times vary depending on temperature, humidity, and film thickness. Typically, the coating will be tack-free in approximately 10 minutes, dry to handle in one hour, and fully cured in 24 hours.

What is the recommended thickness for HumiSeal® 1B12?

The recommended coating thickness for HumiSeal® 1B12 is 25 to 75 microns. This range ensures optimal protection without compromising flexibility or electrical performance. The thickness can be adjusted by controlling viscosity with HumiSeal® Thinner 600 or 601 during application.

What are the differences between application methods for HumiSeal® 1B12?

HumiSeal® 1B12 can be applied via spraying, dipping, or brushing. Spraying and dipping are ideal for large-scale production, while brushing is suited for small repairs. Each method requires adjusting viscosity with the appropriate thinner for a uniform coating.

What is the maximum operating temperature for HumiSeal® 1B12?

HumiSeal® 1B12 can withstand thermal shock from –65°C to +125°C. It is not recommended for continuous operation above 130°C, as prolonged exposure to higher temperatures may degrade its protective properties.

What safety precautions should I take when using HumiSeal® 1B12?

The solvents in HumiSeal® 1B12 are flammable, so avoid open flames or sparks during application. Use in a well-ventilated area to prevent inhalation of vapors or spray mist, and avoid skin and eye contact. Always consult the Safety Data Sheet (SDS) prior to use for detailed safety guidelines.

How can I ensure proper application of HumiSeal® 1B12?

HumiSeal® 1B12 fluoresces under UV light, allowing for easy inspection of coating coverage. After application, use a UV light source to check for uniform coating and ensure there are no missed areas, which is critical for high-reliability electronics manufacturing.

How does HumiSeal® 1B12 perform in harsh environments?

HumiSeal® 1B12 is designed for harsh conditions, with a moisture insulation resistance of 3.0 × 1010 ohms and fungus resistance per ASTM G21. It maintains performance in humid, mechanically stressful, or temperature-cycling environments, making it ideal for mission-critical systems.

Learn More About HumiSeal® 1B12

HumiSeal® 1B12 is a proven solution for engineers seeking long-term protection of electronic assemblies in demanding environments. This acrylic conformal coating offers a unique combination of ease of use, excellent electrical insulation, and mechanical resilience—making it an industry favorite for protecting PCBs in sectors such as automotive, aerospace, consumer electronics, and industrial automation.

Key Features at a Glance

  • ✔ Tack-free in 10 minutes at room temperature
  • ✔ Compatible with “no-clean” flux residues
  • ✔ Low viscosity for easy application
Electrical protection 1B12
UV inspection 1B12

 


Versatile Application Methods 🧰

Application methods

Whether you’re using spraying, dipping, or brushing, 1B12 offers flexibility in manufacturing workflows. It can be diluted with HumiSeal® Thinner 503 or 521 to fine-tune application characteristics based on part geometry and production scale. The coating cures at room temperature in 24 hours, allowing integration into both batch and inline processes.

Application Methods:

  • Spray: Dilute with HumiSeal® Thinner 503 or 521
  • Dip: 5–15 cm/min withdrawal rate
  • Brush: For touch-up applications

Cure the coating at room temperature (24 hrs) for convenience, or accelerate with thermal curing to match fast-paced production cycles.

Application Compatibility

It integrates well with lead-free processes, supports standard cleaning practices, and offers strong performance even on flux-contaminated surfaces.

Compatible With:

  • ✔ Compatible with “no-clean” flux residues
  • ✔ Common PCB finishes including ENIG, HASL, and OSP
  • ✔ High-reliability applications requiring low ionic content
  • ✔ Lead-free and RoHS-compliant manufacturing environments
  • ✔ Cures at room temperature (24 hrs)

Additionally, its UV fluorescence ensures easy inspection, and the coating is reworkable using standard HumiSeal strippers—ideal for repairable designs and serviceable assemblies.


High-Performance Electrical Protection 🧪

1B12 delivers a dielectric breakdown voltage of 1,500 volts and an insulation resistance exceeding 2.5 × 1014 ohms, protecting even the most sensitive circuit designs from moisture, contaminants, and voltage-induced failure. It’s also rated UL 94 V-0, ensuring flame retardancy in critical applications.

Fluorescent for Inspection 💡

To simplify quality assurance, HumiSeal® 1B12 fluoresces under UV light, making it easy to confirm proper coating coverage during post-application inspection—an essential feature for high-reliability electronics manufacturers.

Electrical protection 1B12
UV inspection 1B12

Repairable and Reworkable 🔁

Unlike many conformal coatings, HumiSeal® 1B12 is easily repairable. Should rework or component replacement be required, the coating can be selectively removed using HumiSeal® Stripper 1080 or 1080A, making it ideal for prototyping, low-volume builds, or field serviceability.

Reliable Across Environments 🌍

With a wide thermal shock range of –65°C to +125°C and resistance to fungus (ASTM G21) and moisture, 1B12 ensures consistent performance across varied environmental conditions. It’s particularly well-suited for mission-critical systems exposed to humidity, mechanical stress, or temperature cycling.


Compliance You Can Trust ✅

HumiSeal® 1B12 meets stringent industry standards, ensuring reliability and regulatory adherence for OEMs and contract manufacturers:

  • MIL-I-46058C Qualified
  • RoHS Directive 2002/95/EC Compliant

Leading Brands Trust in Our Products and Services