HUMISEAL 2A13
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- 1:1 Part A-to-Part B Mixing
- 60-Minute Pot Life
- Thermal Shock and Vibration Protection
Product Description
HumiSeal 2A13 is a two-component, low-stress polyurethane encapsulant for electronic sealing and encapsulation. It mixes at 1:1 and cures to a clear, elastic material used for electronic packages exposed to repeated thermal shock and high vibration. Typical component viscosities are 2,700 cP for Part A and 7,500 cP for Part B. Typical processing times are a 60-minute pot life, 120-minute handling time, and full cure after 24 hours at room temperature or one hour at 65 deg C. Substrates include metals, glass, ceramics, and plastics.
Key features
- 1:1 Part A-to-Part B Mixing: Typical component viscosities are 2,700 cP for Part A and 7,500 cP for Part B.
- 60-Minute Pot Life: Typical handling time is 120 minutes under the stated conditions.
- Thermal Shock and Vibration Protection: The cured encapsulant is used for electronics exposed to repeated thermal shock and high vibration.
Applications
Electronic sealing and encapsulation on metals, glass, ceramics, and plastics.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Typical two-component values from the 2018 HumiSeal Encapsulation Solutions brochure; time values may vary with volume or mix ratio.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemistry | Urethane | - | Two-component system; manufacturer brochure |
| Part A viscosity | 2,700 | cP | Typical component value |
| Part B viscosity | 7,500 | cP | Typical component value |
| Mix ratio | 1:1 | - | Part A:Part B; basis not stated |
| Pot life | 60 | minutes | Typical 100 g volume |
| Handling time | 120 | minutes | Typical 100 g volume |
After-processing / final-state properties
Typical cured-system values from the 2018 HumiSeal brochure for the exact 2A13 configuration.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Full cure | 24 hours at RT or 1 hour at 65 deg C | - | Time may vary with volume or mix ratio |
| Cure type | Two-component with heat option | - | Manufacturer brochure |
| Color | Clear | - | Cured system |
| Hardness | Shore D31 | - | Cured system |
| Operating temperature | -50 to 110 | deg C | Cured system |