HUMISEAL UV12

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

HUMISEAL UV12

Main features

  • Fast 30-Second UV Handling
  • Low-Viscosity Optical Encapsulation
  • Water-White LED Encapsulation

Product Description

HumiSeal UV12 is a one-part optical encapsulant that combines low viscosity with fast UV response for LED and light-array applications. Typical viscosity is 2,500 cP, and the water-white urethane/acrylate material remains workable until UV exposure. With a typical UV dose of 1 to 2 J/cm^2, it reaches handling condition in 30 seconds. The clear rigid cured material has Shore D80 hardness and a typical operating-temperature range of -50 to 125 deg C. Its one-part format and transparent final appearance fit LED encapsulation and other optical applications.

Key features

  • Low supplied viscosity: Typical supplied viscosity is 2,500 cP.
  • 30-second UV handling: Handling condition is reached in 30 seconds with UV exposure.
  • Clear rigid cure: The cured material is water-white, clear, and rigid.

Applications

LED encapsulation, optical applications, and light arrays.

Product Family

HUMISEAL UV12

Loading pricing…

Technical Specifications

General Properties
Component System
One
Thermal Properties
Operating Temperature
-50 to 125 °C
Physical Properties
Viscosity
2,500 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical product-selection data and are not specifications.

PropertyValueUnitMethod / condition
Viscosity2,500cPAs supplied; typical
Working timeUntil UV exposureAs supplied; typical
Handling time30secWith UV exposure; typical
UV dose1 to 2J/cm^2UV cure; typical
Technical properties

After-processing / final-state properties

Values describe the UV-cured material and are typical product-selection data, not specifications.

PropertyValueUnitMethod / condition
ColorClearCured material; water-white
HardnessD80Shore DCured material; typical
Operating temperature-50 to 125deg CCured material; typical range

Leading Brands Trust in Our Products and Services