HumiSeal Acrylic Gel Conformal Coating

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

HumiSeal Acrylic Gel Conformal Coating

Main features

  • Thixotropic
  • Fast-drying
  • Easy repairability

Product Description

HumiSeal Acrylic Gel is a fast-drying, single-component acrylic paste engineered for precision and high-build protection. Its thixotropic nature means it stays in place upon application but flows under pressure, making it the perfect companion for standard acrylic conformal coatings. It provides a rugged barrier against moisture and environmental contaminants while remaining easy to rework.

Product Key Features

  • Designed as a thick paste that will not slump or run, allowing for precise placement on vertical surfaces or specific components.
  • Rapid evaporation of solvents speeds up production throughput and allows for quicker handling of assemblies.
  • Easily removed with solvents or a soldering iron, making it ideal for boards requiring field service.

Applications

  • Used to create a physical perimeter (a "dam") on a PCB to prevent liquid conformal coatings from flowing into restricted areas like connectors or test points.
  • Effectively seals the base of large components to prevent moisture ingress or "wicking" underneath parts.
Product Family

HS-AG/55C

55cc Syringe
1. Select Package Size

Loading pricing…

Product availability
EU Shipping in 6 weeks
Packaging
Unit of measure Syringe
Net weight 0.07 kg
Gross weight 0.12 kg
Dimensions 2.5 x 2.5 x 17.3 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.95 g/cm3