LOCTITE STYCAST E2517

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE STYCAST E2517

Main features

  • Low CTE
  • Low Viscosity
  • High temperature resistance

Product Description

LOCTITE® STYCAST E 2517 epoxy encapsulant is formulated for use on bare chip protection in a variety of advanced packages where ease of flow and high thermal stability are required.

Recommended Cure Schedule

  • Precure 1 hour @ 120°C
  • Full cure 1 hour @ 150°C
  • Post cure 2 hours @ 200°C
Product Family

E2517/30C0

30 CC Syringe - 1293896
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 20 days
Packaging
Unit of measure Syringe
Net weight 40 g
Gross weight 61 g
Dimensions 4 x 3 x 11.8 cm
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
220 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.5 W/m.K
Chemical Properties
Water Absorption
0.08 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
22,500 mPa.s