TGP 6000PT | Thermal Putty Pad

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

TGP 6000PT | Thermal Putty Pad

Main features

  • 0.27 Thermal Impedance
  • 6.0 Thermal Conductivity
  • 0.5 - 5 mm Thickness

Product Description

Honeywell TGP 6000PT Thermally Conductive Putty Pads provide high thermal performance and excellent thermal reliability. The material’s putty-like design enables excellent gap-filling capability for applications with large dimensional variances. Special surface reinforcement enables easier handling for operators during high volume assembly. It comes contained and reinforced within single sided fiber glass  and dual liners. 

Honeywell TGP 6000PT is naturally tacky and requires no additional adhesive to mate to heat source and heat sink. This product can replace thermal grease and improve dripping and pump out. It is available in thicknesses ranging from 1.0mm to 5.0mm.

Need a thickness below 1mm? Then we recommend our standard Thermal gap pads.

Product Family

TGP6000PT/1P0

457 x 457 x 1.0mm Pad
1. Select Package Type
2. Select Version

Loading pricing…

Product availability
EU Shipping in 16 weeks
Packaging
Unit of measure Pad
Net weight 0.71 kg
Gross weight 0.78 kg
Dimensions 45.7 x 45.7 x 0.1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Gray
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
1 - 5 mm
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
3.4
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
6.0 W/m.K
Thermal Impedance
0.27 °C·cm²/W
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
4000000000000000 Ohms⋅cm

Additional Information

Fiberglass Layer Solutions:

Since these are ultra-soft materials, handling during application presented certain challenges. To improve stability and ease of processing, multiple fiberglass reinforcement solutions was added.
We can provide below versions for customers’ consideration.

TGP6000PT: 2 layers of fiberglass
TGP6000PT-01: 1 layers of fiberglass
TGP6000PT-00: No fiberglass



Shelf Life: 12 months at 23±2˚C

Thickness range: 1.0-5.0mm with 0.25mm incremental

Thickness Tolerance: >=1mm, ±10%, 0.5-1mm, ±0.1mm

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers