TGP3000E | Thermal Gap Pad

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

TGP3000E | Thermal Gap Pad

Main features

  • 0.65 Thermal Impedance
  • 3.0 Thermal Conductivity
  • Excellent surface wetting

Product Description

Honeywell TGP3000E Thermal Gap Filler Pads provide high thermal performance with ease of use across multitude of applications. Its ultra-high compressibility enables low stress and excellent conformity to mating surfaces. It is designed to minimize thermal resistance at interfaces, and maintain excellent performance through reliability testing.

Honeywell TGP3000E is naturally tacky, and requires no additional adhesive which could inhibit thermal performance. Even though these pads come in large dimensions, it is suggested to cut and apply them in smaller pieces to ensure part uniformity and to avoid any issues related to their application. Products are available in a thickness range from 0.5mm to 5.0mm.

Product Key Features

  • Thermally Conductive (3.0W/m•K) — better heat dissipation
  • Ultra-high compressibility for low stress applications
  • Excellent surface wetting for low contact resistance.

Applications

  • Semiconductor logics & memory
  • Power devices and modules
  • Consumer electronics, telecommunications, and automotive electronics

 

Product Family

TGP3000E/1P40.6

40.6 x 18.3 x 1mm Pad
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 16 weeks
Packaging
Unit of measure Pad
Net weight 2.154642 g
Gross weight 2.154642 g
Dimensions 1.83 x 4.06 x 0.1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Green
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.9
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.0 W/m.K
Thermal Impedance
0.5 °C·cm²/W
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
3000 V
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1000000000000000 Ohms⋅cm

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers