TG1500I | Thermal Grease

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

TG1500I | Thermal Grease

Main features

  • 0.03 Thermal Impedance
  • 1.5 Thermal Conductivity
  • 30μm BLT

Product Description

TG1500I Thermal Silicone Grease offers a thermal conductivity of 1.5 W/mK and a controlled bond line thickness of 30 micron @35psi, 50oC.  Its viscosity and excellent thixotropy make it fit for large–scale production with dispensing, screen printing and stencil printing. It is an excellent, option for thermally demanding applications that can support a >30um BLT.

TG1500I is used for applications with high power density requirements. It provides superior thermal performance with ease of use across a multitude of applications.  It is a stable homogeneous mixture under room temperature with an operating temperature range of -40oC to 150oC. Please note that this thermal grease contains solvent and requires a drying step.

Product Key Features:

  • Low thermal resistance (0.021°C-in²/W at 50 psi) — effectively address overheating and reliability issues
  • Maintains high reliability and performance across demanding environments and applications
  • Suitable for use in pneumatic dispensing and screen printing systems, supporting automated and high-volume manufacturing

Applications

  • Heat dissipation from heat-generating components (like CPUs and GPUs) to cooling solutions (like heat sinks).
Product Family

TG1500I/1J0

1Kg Jar
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 10 x 8 x 8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
White
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.7
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.5 W/m.K
Thermal Impedance
0.03 °C·cm²/W
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
10000000000000 Ohms⋅cm
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
250000 mPa.s

Leading Brands Trust in Our Products and Services