Honeywell TA 3000

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Honeywell TA 3000 Honeywell TA 3000

Main features

  • Moisture cure
  • Good thermal performance
  • Adjusts to irregular surfaces

Product Description

Honeywell TA3000 is a one-part moisture cured silicone thermally conductive adhesive, used to bond the heat generating component with heat sink when exposure to moisture in the air. The cured material could function as excellent heat transfer media, fixing of electronic components and sealing protection against contaminants at the same time during application.

Honeywell TA 3000 is a room temperature vulcanization adhesive that forms a curable adhesion layer between two surfaces with a little pressure and meanwhile offer good heat dissipation effect in use across multitude of applications. It exhibits a linear CTE of 102 ppm/°C and 10-20min of tack free time in room temperature.

Honeywell TA 3000 can be used with manual or automatic dispense and cures at room temperature with 10-80% realtive humidity. It is not suggested to use it at highly confined or deep sections spaces and it is typically used for PCBA, LED assemblies, power units and automotive electronics.

Product Family

TA3000/300C0

300cc Al cartridge

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
White
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.8
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3 W/m.K
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
440,000 mPa.s

Leading Brands Trust in Our Products and Services