Main features

  • Dark Red
  • 3.5 Thermal Conductivity
  • High flow rate

Product Description

HT3500 silicone based one-part Gap Filler - thermal gel provides a thermal conductivity of 3.5 W/mK along with high conformability and high compressibility. It is formulated to deliver high dispense rates for improved productivity, long-term reliability performance and easy reworkability.

HT3500 is designed to minimize thermal resistance at interfaces, maintain excellent performance through reliability testing, and provide scalable application at a competitive cost. The minimum bondline thickness that it can reach is 0.1mm with a Thermal Impedance of 0.4. Additionally it performs great in oil,crack and slump testing and it exhibits no pump out and cracking risk. This is the most popular, commercial version of the material but we also provide the LV (low volatile) version for specific applications such as optical that might require i.e less clouding.

HT3500 has a high flow rate, above 15 g/min, high breakdown strength (above 5 kV/mm) and very low out gassing (below 0.5%)

Product Family

HT3500/300C0

300cc Al cartridge
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Cartridge
Net weight 0.96 kg
Gross weight 1.06 kg
Dimensions 22 x 4.7 x 4.7 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Dark Red
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
3.2
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.5 W/m.K
Thermal Impedance
0.35 °C·cm²/W