MOLYKOTE L-1568
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Lower-Viscosity Process-Gas Lubrication
- Wide-Range PAO Viscosity Control
- Defined Oxygen-Service Limit
Product Description
MOLYKOTE L-1568 Process Gas Oil is an ISO VG 68 PAO process-gas oil for compressors and vacuum pumps handling corrosive gases such as hydrogen chloride or methyl chloride. It has typical kinematic viscosity of 68 cSt at 40 deg C and 10 cSt at 100 deg C, with a viscosity index of 140. The specialized formulation includes a C1 additive package. Because the oil is not formulated with antioxidants, total oxygen should be no more than 2% of the gas stream. This lower-viscosity grade is for the specified process-gas service.
Key features
- ISO VG 68 Process-Gas Profile: Typical viscosity is 68 cSt at 40 deg C for lower-viscosity process-gas lubrication.
- Corrosive-Gas Application: The oil is intended for compressors or vacuum pumps handling hydrogen chloride or methyl chloride.
- Gas-Stream Oxygen Limit: Total oxygen should be no more than 2% of the gas stream.
Applications
Process-gas compressors; highly corrosive or reactive gas service including hydrogen chloride and methyl chloride; vacuum pumps where specified by the manufacturer.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Typical values; not for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| ISO viscosity grade | 68 | - | Manufacturer designation |
| Kinematic viscosity | 68 | cSt | Typical at 40 deg C |
| Kinematic viscosity | 10 | cSt | Typical at 100 deg C |
| Viscosity index | 140 | - | Typical |
| Pour point | -30 | deg C | Typical |
| Specific gravity | 0.834 | - | Typical at 20 deg C |
| Base oil | PAO | - | Typical composition |
| Additive package | C1 | - | Manufacturer designation |