MOLYKOTE L-1510

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

MOLYKOTE L-1510

Main features

  • Corrosive-Gas Compressor Lubrication
  • Wide-Range ISO VG 100 Stability
  • Clear Oxygen-Service Boundary

Product Description

MOLYKOTE L-1510 Process Gas Oil is an ISO VG 100 PAO process-gas oil for compressors or vacuum pumps handling corrosive gases, including hydrogen chloride and methyl chloride. Typical kinematic viscosity is 100 cSt at 40 deg C and 14 cSt at 100 deg C, with a viscosity index of 138. The formulation includes a C1 additive package. Because the oil is not formulated with antioxidants, total oxygen should be no more than 2% of the gas stream.

Key features

  • Corrosive-Gas Service: The process-gas formulation is intended for compressors or vacuum pumps handling hydrogen chloride or methyl chloride.
  • ISO VG 100 PAO Profile: Typical viscosity is 100 cSt at 40 deg C and 14 cSt at 100 deg C.
  • Gas-Stream Oxygen Limit: Total oxygen is limited to no more than 2% of the gas stream.

Applications

Process-gas compressors; highly corrosive or reactive gas service including hydrogen chloride and methyl chloride; vacuum pumps where specified by the manufacturer.

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.838

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values; not for use in preparing specifications.

PropertyValueUnitMethod / condition
ISO viscosity grade100-Manufacturer designation
Kinematic viscosity100cStTypical at 40 deg C
Kinematic viscosity14cStTypical at 100 deg C
Viscosity index138-Typical
Pour point-30deg CTypical
Specific gravity0.838-Typical at 20 deg C
Base oilPAO-Typical composition
Additive packageC1-Manufacturer designation