LORD® 810S/20GB Flexible Acrylic Adhesive System

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ORD® 810S/20GB Flexible Acrylic Adhesive System

Main features

  • 2:1 mix ratio acrylic adhesive system
  • 8-12 minute selectable working time
  • Non-sag structural bonding with environmental and solvent resistance.

Product Description

LORD® 810S paired with LORD Accelerator 20GB, creates a high-performance, flexible acrylic adhesive system specifically engineered for thin-gauge substrates. This "Low Read-Through" (LRT) formula is designed to bond metals and engineered plastics without the surface distortions or "ghosting" typically caused by exothermic heat during the curing process. By incorporating specialized glass beads, LORD®810S/20GB ensures a uniform, controlled bondline thickness every time, making it the premier choice for visible, high-aesthetic assemblies.

Product Key Features

  • Superior Aesthetics (LRT) – bonds thin and flexible substrates with little to no bondline read-through.
  • Precision Bondline Control – contains integrated glass beads in the Accelerator 20GB to maintain exact adhesive thickness and prevent over-clamping.
  • Non-Sag - remains in place on vertical or overhead surfaces to support bead control during assembly.
  • Environmental Resistance - cured adhesive resists weathering, humidity, salt spray, and many solvents.

Applications

This adhesive fits composite and mixed-material assemblies that require structural bonding, controlled bead placement, and curative options matched to production timing.

  • Thin-Gauge Metal Assembly: bonding aluminum and galvanized steel panels where welding would cause warping or require extensive post-finishing.
  • Engineered Plastics: provides high-strength, flexible bonds for materials like PC-ABS and other plastics with simple cleaning.
  • Outdoor & Industrial Equipment: resists weathering, indirect UV exposure, dilute acids, and solvents, making it ideal for enclosures and exterior signage.
Product Family

PL-810S/50ML

50mL Cartridge - Black
1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Cartridge
Net weight 50 g
Gross weight 55 g
Dimensions 6 x 6 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black Paste
Density (g)
0.935-0.970 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
2:1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
40000-130000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
15 °C
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
43 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
190 %

Additional Information

Low Read-Through (LRT) Acrylic Adhesive System

LORD® 810S / Accelerator 20GB

LORD® 810S is a flexible, Low Read-Through (LRT) acrylic adhesive system specifically engineered for bonding thin-gauge metals and engineered plastics like PC-ABS. When paired with LORD Accelerator 20GB, it provides high-speed structural bonding with minimal surface distortion. The system features integrated glass beads for precise bondline control and excels at cutting through mill oils, reducing the need for extensive substrate preparation.

2:1 mix ratio by volume 30 min handling strength Low-odor formula Integrated Glass Beads
Contact Us
LORD 810S product package
LORD® 810S LRT System 

Key Features

  • Aesthetics: Bonds thin substrates with little to no bondline read-through (BLRT).
  • Integrated Glass Beads: Accelerator 20GB ensures precise and consistent bondline thickness.
  • Low Prep: Excellent adhesion to "as-received" metals with standard mill oils.
  • Fast Cure: Achieves 90% strength in 30 minutes at room temperature.
  • Resilience: Resists dilute acids, solvents, UV exposure, and weathering.

Processing Summary

Mix ratio: 2:1 Adhesive to Accelerator by volume. Visual confirmation via even color distribution.
Cure Timing: 90% strength at 30 minutes; full cure at 24 hours @ 77°F (25°C).
Temperature Range: Maintains performance from -40°F to +300°F (-40°C to +149°C).
Rheology: Non-sag paste remains in position on vertical and overhead surfaces.
Typical Properties

Adhesive

Data is typical and not to be used for specification purposes.

Property LORD® 810S Condition / method
Appearance Black Paste Observation
Viscosity 40,000 -130,000 cP Brookfield, @ 77°F (25°C)
Density 7.8 - 8.1 lb/gal (935 - 970 kg/m³) -
Flash point >59°F (>15°C) Closed cup

Adhesive Mixed with Recommended Accelerator

Data is typical and not to be used for specification purposes.

Property LORD® 810S Condition / method
Mix Ratio, Adhesive to Accelerator by Weight/ by Volume 1.1:1/ 2:1 -
Working Time 8-12 minutes @ 70°F (21°C)
Time to Handling Strength 20-25 minutes @ 70°F (21°C)
Mixed Appearance Dark Grey Paste Observation
Cured Appearance Dark Grey Observation

Typical Cured Properties

Cured for 24 hours at room temperature. Data is typical and not to be used for specification purposes.

Property LORD® 810S Condition / method
Hardness (Shore D) 40 -
Tensile Strength at Break 2088 psi (14.4 MPa) -
Elongation 190 % -
Glass Transition Temperature (Tg) 136°F (58°C) -

Typical Post-Baked Properties

Cured for 24 hours at room temperature then baked at 140°F (60°C) for 500 hours. Data is typical and not to be used for specification purposes.

Property LORD® 810S Condition / method
Hardness (Shore D) 69 -
Tensile Strength at Break 2088 psi (14.4 MPa) -
Elongation 22 % -
Glass Transition Temperature (Tg) 136°F (58°C) -
Storage and handling (per technical data sheet)
Shelf life is one year when stored below 77°F (25°C) in original, unopened container. Storage temperatures of 40-60°F (4-15°C) are recommended. If stored cold, allow product to return to room temperature before using. Protect from exposure to direct sunlight.
LORD 810S adhesive is flammable. Do not store or use near heat, sparks or open flame.
Applications

Where LORD® 810S Fits

ACM Panel bonding
ACM & Signage Bonding
Specifically engineered for Aluminum Composite Material (ACM) where finishing aesthetics are important and bondline read-through must be eliminated.
  • Low Read-Through (LRT) preserves smooth exterior surfaces.
  • Glass beads in Accelerator 20GB ensure precise bondline thickness.
  • Excellent resistance to UV exposure and weathering.
Architectural panel assembly
Architectural Facades
Ideal for bonding thin-gauge galvanized steel, aluminum, and cold-rolled steel (CRS) panels to frames without the need for mechanical fasteners.
  • Non-sag formula supports vertical and overhead assembly.
  • Minimal substrate prep required for metals and plastics.
  • Maintains performance from -40°F to +300°F.
Plastic enclosure assembly
Plastic & Hybrid Enclosures
A flexible, toughened solution for bonding engineered plastics like PC-ABS to metal frames in medical or electronic housings.
  • Fast cure speed for high-throughput production lines.
  • Resistant to solvents, greases, and moisture.
  • Flexible system absorbs thermal expansion differences.
Product Demo

Using LORD® 810S

Practical view of cartridge dispensing, bead placement, part mating, and assembly handling for the LORD® 810S system.

Handling and Application Guidance

Process Notes 

Surface Preparation
  • Remove grease, dirt, and poorly adhering oxides.
  • Mill oils typically do not require removal for metal bonding.
  • Plastics usually require simple cleaning; some may need abrasion.
Mixing and Dispensing
  • Ensure 2:1 ratio (Adhesive:Accelerator).
  • Level plungers before attaching mixer.
  • Handheld cartridges or meter/mix equipment are compatible.
Cleanup and Teardown
  • Clean uncured adhesive with IPA, Acetone, or MEK.
  • To separate cured parts, heat to 400°F (204°C) to soften the bond.
Next Steps

Ready to Qualify with LORD® 810S?

Achieve flawless aesthetics and structural integrity on thin substrates. Share your application details and we will help you configure the LORD 810S / 20GB system for your production line.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers