LOCTITE SI 5421

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK SI 5421

Main features

  • Room temperature cure
  • Low stress
  • EMI Shielding gasketing material

Product Description

LOCTITE SI 5421, Silicone, Bonding or Gasketing, Flexible, Formed-in-place, Electrically Conductive Adhesive. It enhances the load bearing & shock absorbing characteristics of the bond area.

LOCTITE SI 5421 is used for automotive sensor bonding and gasketing of EMI/RF shielded enclosures. It is a room temperature vulcanizing adhesive that moisture cures in 24h to make a flexible, formed-in-place, electrically conductive bond.

Surface Cure

  • LOCTITE SI 5421 becomes tack free on exposure to atmospheric moisture within 1 hour at 23±2°C / 50±5%RH.
Product Family

SI5421/50X0

50ml jar - 236637
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Unit of measure Jar
Net weight 160 g
Gross weight 247 g
Dimensions 4 x 4 x 9.9 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
3.05
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.81 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.01 Ohms⋅cm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
40 %