LOCTITE SF 7515
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- No-Rinse Spray or Wipe
- 20 to 40 deg C Application
- Aluminum, Zinc, and Steel Pretreatment
Product Description
LOCTITE SF 7515 is a one-part, amber, water-based surface treatment for temporary flash-rust protection and metal pretreatment before coating. Supported metal surfaces include aluminum, zinc, zinc alloy, cold-rolled steel, and blasted metal. Apply the no-rinse treatment by spray or wipe to a clean surface at 20 to 40 deg C. Remove excess as needed and allow the thin film to dry. Typical as-supplied density is 1.01 g/cm^3 and pH is 2.1 to 2.7.
Key features
- No-Rinse Spray or Wipe: Apply to clean metal, remove excess as needed, and allow the film to dry without rinsing.
- Temperature-Controlled Application: Apply at 20 to 40 deg C.
- Aluminum, Zinc, and Steel Pretreatment: Supported surfaces include aluminum, zinc, zinc alloy, cold-rolled steel, and blasted metal.
Applications
Temporary flash-rust protection and metal pretreatment before coating on aluminum, zinc, zinc alloy, cold-rolled steel, and blasted metal surfaces.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As supplied
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Amber liquid | TDS; as supplied | |
| Density | 1.01 | g/cm^3 | Typical TDS value |
| pH | 2.1 to 2.7 | Typical TDS value |