LOCTITE M4100 E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE M4100 E&C

Main features

  • Conductive
  • screen printable
  • Electroless nickel plateable

Product Description

LOCTITE M 4100 MINICO E&C electroless nickel plateable conductive polymer is designed as a terminator where the M2000 RS MINICO E&C polymer resistor series has been applied.

LOCTITE M 4100 MINICO E&C is designed to be applied using standard screen printing methods.

Product Family

M4100/0.4KJ

0.4kg jar - 1239161
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 131 days
CA Shipping in 8 weeks
EU Shipping in 60 days
Packaging
Unit of measure Jar
Net weight 400 g
Gross weight 470 g
Dimensions 8.2 x 8.2 x 7.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
2800000 g/cm3
Solids
78 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
45 mPa.s

Additional Information

Storage
Store product in the unopened container in a dry location. Storage information may be indicated on the product container labeling.

Store in a cool, well ventilated area.

Optimal Storage : 18 to 25 °C


Material removed from containers may be contaminated during use. Do not return product to the original container. Henkel Corporation cannot assume responsibility for product which has been contaminated or stored under conditions other than those previously indicated. 