LOCTITE EDAG PM 406V1 E&C
Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category
Main features
- High conductivity
- High solids content
- Hot air dry cure
Product Description
LOCTITE EDAG PM406V1 E&C is a screen printable, conductive ink formulated to have very high conductivity and solids content. It can be used on PET, paper and PVC substrates.
LOCTITE EDAG PM406V1 E&C can operate in operating temperature up to 100°C that has high solids content and dries fast. It is typically used for printed circuitry, RFID and other conductive circuits.
Recommended Drying Cycle
- 30 minutes @ 90°C or
- 15 minutes @ 120°C
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.616 kg
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Density (g)
3 g/cm3
Solids
79 %
Physical Properties
Viscosity
21,600 mPa.s
Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application