Main features

  • Good dielectric strength
  • Excellent printability
  • Fast UV Cure

Product Description

LOCTITE EDAG PF 455BC E&C is a translucent UV curable acrylate that is formulated as a crossover dielectric and is compatible with other EDAG E&C inks. Mainly used as a dielectric ink.

LOCTITE EDAG PF 455BC is resistant to humidity, has excellent printability and adheres well to both treated and untreated polyester film substrates.  It has good dielectric strength and is compatible for use with ElectroDAG conductive and dielectric polymer thick film inks.  

UV Cure 

  • UV lamp 80Watt/cm or
  • UV lamp 120Watt/cm
Product Family

PF455BC/1J0

1Kg Jar - 1263294
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.449 kg
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
1,02 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
13,500 mPa.s

Additional Information

Recommended UV Cure Condition
UV lamp 80Watt/cm or
UV lamp 120Watt/cm
When applying LOCTITE EDAG PF 455BC E&C as a crossover, two layers of approximately 12 to 15μm each should be applied. Cure both layers at an energy level of 0.5Joule/cm2 to obtain a good inter- coat adhesion between the first and second layer and to obtain a maximum adhesion of the crossover.
When using LOCTITE EDAG PF 455BC E&C as a crossover, be sure to dry the inks printed over it within 5 minutes. Do not let the inks printed over LOCTITE EDAG PF 455BC E&C air dry for extended periods of time.