LOCTITE EDAG PF 455B E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE EDAG PF 455B E&C

Main features

  • Non conductive
  • Dielectric crossover
  • Fast UV Cure

Product Description

LOCTITE EDAG PF 455B E&C UV curable acrylate is formulated as a crossover dielectric and is compatible with other EDAG E&C inks. It is a translucent green acrylate that is usually used in combination with other inks to enhance the end properties.

LOCTITE EDAG PF 455B E&C has excellent adhesion and printability along with good dielectric strength. It is typically used as an insulating crossover in assembly operations. For example it can be used as a dielectric ink to make a bridge over conductive inks such as ECI 1010 AND ECI 1011.

UV Cure 

  • UV lamp 80Watt/cm or
  • UV lamp 120Watt/cm 
Product Family

PF455B/1JO

1Kg Jar - 1263298
1. Select Package Type

Loading pricing…

Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 2.546 kg
TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
13,500 mPa.s
General Properties
Density (g)
1,02 g/cm3

Additional Information

Recommended UV Cure Condition
UV lamp 80Watt/cm or
UV lamp 120Watt/cm

When applying LOCTITE EDAG PF 455B E&C as a crossover, two layers of approximately 12 to 15μm each should be applied. Cure both layers at an energy level of 0.5Joule/cm2 to obtain a good inter-
coat adhesion between the first and second layer and to obtain a maximum adhesion of the crossover.
When using LOCTITE EDAG PF 455B E&C as a crossover, be sure to dry the inks printed over it within 5 minutes. Do not let the inks
printed over LOCTITE EDAG PF 455B E&C air dry for extended periods of time.

Leading Brands Trust in Our Products and Services