LOCTITE EDAG PF 407C E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE EDAG PF 407C E&C

Main features

  • Screen printable
  • Extended screen residence time
  • Carbon filled

Product Description

LOCTITE EDAG PF407C E&C polymer thick film is designed for production of low voltage circuitry on polyester film and solvent sensitive substrates such as polycarbonate. It can be used in continuous operating temperatures as high as 105°C and it typically used for printed resistors, membrane touch switches, heating elements, flexible circuits and protection against electrostatic discharge (ESD).

LOCTITE EDAG PF407C E&C is a conductive, screen printable thermoplastic with extended screen residence time over EDAG PF 407A E&C. It has good adhesion and flexible, low temperature drying cycles. This ink works on substrates such as Polyester, Polyimide, Polycarbonate, paper and cardboard.

Drying Cycle

  • 30 minutes @ 90°C or
  • 15 minutes @ 120°C

LOCTITE EDAG PF 407C E&C can be dried immediately after printing.

Product Family

PF407C/1B0

1Kg Jar- 1239174
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 30 days
Packaging
Unit of measure Bottle
Net weight 1 kg
Gross weight 1.15 kg
Dimensions 11.2 x 11.2 x 16.3 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
37 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
42,500 mPa.s

Additional Information

Optimal Storage : 5 to 30 °C

 

TYPICAL SCREEN PRINTING PROCESS
Recommended Thickness
-Applied dry coating thickness , μm 6 to 10


Emulsion Thickness
-Emulsion Thickness , μm 20 to 40

Recommended Squeegee
-Polyurethane , durometer 70 to 75

Recommended Screen Type
-Monofilament polyester screen, threads/cm 61 to 90
-Stainless steel screen , threads/cm 77 to 110

Printing Equipment Type
-Manual
-Semi-automatic
-High speed reel-to-reel