LOCTITE EDAG PF 407A E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE EDAG PF 407A E&C

Main features

  • Print Contact areas
  • Good screen residence time
  • Carbon filled

Product Description

LOCTITE EDAG PF 407A E&C is a carbon filled ink with inert pigment that can be used to print contact areas on flexible circuits.  

LOCTITE EDAG PF 407A is a screen printable, conductive, carbon filled thermoplastic with good screen residence time that is flexible for low temperature drying cycles.

LOCTITE EDAG PF 407A is typically used for printed resistors, membrane touch switches. keyboards, heating elements, flexible circuits and ESD protection. It can continuously operate at a temperature of 105°C and has been successfully used on Polyester, Polyimide, Polycarbonate, paper and cardboard substrates.

Drying Cycle

  • 30 minutes @ 90°C or
  • 15 minutes @ 120°C
Product Family

PF407A/1J0

1Kg Jar - 1239125
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 30 days
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.15 kg
Dimensions 11.2 x 11.2 x 16.3 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
1,12 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
35,000 mPa.s

Additional Information

Optimal Storage : 5 to 30 °C

 

TYPICAL SCREEN PRINTING PROCESS
Recommended Thickness
-Applied dry coating thickness , μm 6 to 10


Emulsion Thickness
-Emulsion Thickness , μm 20 to 40

Recommended Squeegee
-Polyurethane , durometer 70 to 75

Recommended Screen Type
-Monofilament polyester screen, threads/cm 61 to 90
-Stainless steel screen , threads/cm 77 to 110

Printing Equipment Type
-Manual
-Semi-automatic
-High speed reel-to-reel

Leading Brands Trust in Our Products and Services