LOCTITE EDAG 461SS E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE EDAG 461SS E&C

Main features

  • Conductive
  • Screen printable
  • Dries at low temperatures

Product Description

LOCTITE EDAG 461SS E&C conductive ink is designed for display applications on ITO film. It consists of very finely divided silver particles dispersed in a thermoplastic resin.

LOCTITE EDAG 461SS E&C is a screen printable and extremely flexible polyester resin with a butyl cellosolve acetate. It is typically used on ITO coated films, membrane switches, digitizers and flexible circuits with a maximum operating temperature of 149°C

 

Cure Schedule

  • 30 minutes @ 71°C or
  • 15 minutes @ 93°C or
  • 5 minutes @ 121°C

 

 

Product Family

461SS/1.5J0

1.5Kg Jar - 1224967
1. Select Package Type

Loading pricing…

Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.066 kg
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
75 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
17,000 mPa.s