LINQSOL EMC-9070 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LINQSOL EMC-9070 | Molding compound for high MSL qfn packages LINQSOL EMC-9070 | Black Epoxy Mold Compound

Main features

  • MSL1 260°C
  • Designed for QFN and DFN packages
  • Moisture Corrosion Resistance

Product Description

LINQSOL EMC-9070 is a black semiconductor-grade epoxy molding compound designed for the encapsulation and protection of quad-flat no-leads (QFN) and dual-flat no-leads (DFN). Once molded and post-mold cured, this product provides optimum protection and reliability for these semiconductor devices.

LINQSOL EMC-9070 is a spherical silica filled (89%) EMC, typically used for QFN and DFN packages. QFN and DFN packages are low-profile packages that are MAP molded. This means that the packages are molded together in one large mold and then separated by cutting through the entire package. Epoxy molding compounds made for these types of packages must have a low warpage, and EMC-9070 is no exception. This product is formulated to have very low internal stress to reduce warpage, as well as low moisture absorption to increase MSL performance.

Key Features:

  • JEDEC MSL 1 @260°C
  • Low CTE (8ppm) and mold shrinkage (<0.2%)
  • Low moisture absorption (0.33% after PCT 96hrs@121°C)
  • Halogen-free (contains no br, Sb, P, etc.)
  • REACH and RoHS compliant
  • UL 94 V-0 Flammability 

Application: QFN and DFN Packages

Product Family

EMC-9070/14M4.4G10K

Pelletized - 14MM X 4.4GR | 10kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 11 kg
Dimensions 25 x 25 x 25 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
black
Filler Content
89 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.01
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
126 °C
Mechanical Properties
Molded Shrinkage
0.2 %
Chemical Properties
Moisture absorption
0.33 %
Physical Properties
Spiral Flow @ 175°C
127 cm

Additional Information

PROPERTIES UNITS EMC-9070 EMC-9070SF EMC-9070P
Epoxy Type - Biphenyl Biphenyl Biphenyl
Hardener Type - Hydrophobic Hydrophobic Hydrophobic
Flame Retardant - Metal Hydroxide Metal Hydroxide Metal Hydroxide
Filler Content % 89 86 86.5
Filler Sieved Size um 75 75 75
Specific Gravity - 2.01 1.96 1.98
Spiral Flow @175°C inches 50 79 54
Gel Time @175°C seconds 35 40 24
Glass Transition Temperature °C 126 126 126
CTE by TMA, α1 ppm/°C 8 13 11
CTE by TMA, α2 ppm/°C 30 45 39
Hot Hardness, 120 sec@175°C Shore D 83 79 85
Flexural Strength @25°C MPa 160 113 158
Flexural Modulus @25°C GPa 26 21 23
Moisture Absorption, PCT 96hrs@121°C % 0.33 0.40 0.40
Mold Shrinkage % <0.2 <0.3 <0.3

Ionic Impurities (20hrs @160°C)

pH

Na+

Cl-

 

 -

ppm

ppm

 

6.8

6.7

4.1

 

6.9

7.3

4.0

 

6.9

7.2

4.0

Comments   General product for most QFN packages Long spiral flow with good warpage control for large L/F and panel Short gel time with good warpage control for productivity

 