LINQSOL EMC-7560 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LINQSOL EMC-7560 | Black Epoxy Mold Compound LINQSOL EMC-7560 | Black Epoxy Mold Compound

Main features

  • High Glass Transition Temperature (205 °C)
  • Designed for high voltage, high power discrete packages
  • New Epoxy System To Pass HTRB Tests

Product Description

LINQSOL EMC-7560 is a black, halogen-free epoxy molding compound designed for high-voltage and high-temperature semiconductor applications. It adopts a multifunctional epoxy system with a hydrophobic hardener and a new type of stress modifier that utilizes a super dispersion technology. With a high glass transition temperature (Tg = 205 °C), low coefficient of thermal expansion (CTE), and low modulus, EMC-7560 ensures robust performance. EMC-7560 boasts low moisture absorption (<0.1%) and minimal mold shrinkage, improving reliability. It has a UL 94 V-0 flammability rating, highlighting its adherence to stringent safety standards for high-power semiconductor applications.

LINQSOL EMC-7560 finds its niche in high-voltage and high-power discrete packages, including but not limited to TO220, TO247, and other surface mount devices. It enables SiC power modules to pass and perform well in H(3)TRB, HTGB, and HTOL tests. Its innovative epoxy system, which features a high-density molecule matrix, minimizes ion diffusion, ensuring enhanced reliability and superior performance in challenging HTRB and H3TRB conditions. This material has a CTI of 600V.

Key Features:

  • High temperature stability with high Tg (205 °C) 
  • Excellent electrical stability due to low ion content and mobility
  • Low stress with low CTE (10 ppm) and low modulus
  • Low moisture absorption and low mold shrinkage (<0.1%)
  • Halogen-free (does not contain Br, Sb, P)
  • UL 94 V-0 Flammability 

Application: SiC MOSFETs; TO-package Devices

Product Family

EMC-7560/14M4.4G10K

Pelletized - 14MM X 4.4GR | 10kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 11 kg
Dimensions 25 x 25 x 25 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
black
Filler Content
85 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.95
Chemical Properties
Moisture absorption
0.4 %
Physical Properties
Spiral Flow @ 175°C
82 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
205 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.9 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Mechanical Properties
Molded Shrinkage
0.1 %

Additional Information