LINQSOL EMC-7535MF | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LINQSOL EMC-7535MF | High Tg Mold Compound

Main features

  • Green molding compound
  • Designed for high-power TO packages
  • High Tg, low water absorption, low modulus, and excellent thermal stability

Product Description

LINQSOL EMC-7535MF is a green epoxy molding compound specifically developed for high-voltage and high-power semiconductor devices. It offers low modulus to meet low-stress requirements. With a high glass transition temperature (Tg = 215 °C), minimal moisture absorption, a high comparative tracking index (CTI = 600 V), and a UL 94 V-0 flammability rating highlighting its adherence to stringent safety standards for high-power semiconductor applications,  EMC-7535MF guarantees strong performance and outstanding reliability.

Overall, LINQSOL EMC-7535MF seamlessly integrates advanced material properties, safety compliance, and superior performance, precisely meeting the stringent demands of high-power semiconductor components such as TO packages. LINQSOL EMC-7535MF finds its niche in high-voltage and high-power discrete packages and power modules, including but not limited to IGBT, TO220, TO247, and other surface mount devices.

LINQSOL EMC-7535MF proved its reliability in customers' small SiC discretes—zero voids, zero delamination on Ni-plated Cu leadframes—even after thermal cycles (−40 °C ↔ +125 °C).

 

Key Features:

  • High-temperature stability with high Tg (215 °C) 
  • Excellent electrical stability due to low ion content and mobility
  • Low stress with low CTE (9 ppm) and low modulus (15GPa)
  • Low moisture absorption and low mold shrinkage (0.22%)
  • Halogen-free (does not contain Br, Sb, P)
  • UL 94 V-0 Flammability 

Application: SiC MOSFETs; TO-package Devices, IGBT Modules

Product Family

EMC-7535MF/20M17G15K

Pelletized - 20MM X 17GR | 15kg box
1. Select Package Type
2. Select Product Form
3. Select Pellet Size
4. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 15.5 kg
Dimensions 30 x 30 x 30 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
84 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.96
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
33000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
≤ 0.35 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
215 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.8 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Mechanical Properties
Molded Shrinkage
0.22 %
Curing Conditions
Transfer Pressure
40-90 kg/cm2
Transfer Time
10-25 s
Physical Properties
Spiral Flow @ 175°C
85 cm
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
44000 mPa.s

Additional Information

Processing Instructions

  • Before use, let LINQSOL EMC-7535MF reach room temperature for 24 hours. Keep the bag unopened and stored in a dry location with a relative humidity of ≤50% during thawing to prevent moisture contamination. 
  • Use the materials within 72 hours after removing the container from cold storage.

Storage and Handling

LINQSOL EMC-7535MF is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life at 5 °C is 183 days.

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers