LINQSOL EMC-7535 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

EMC-7535 | Black Epoxy Mold Compound

Main features

  • Green molding compound
  • Designed for high-power TO packages
  • High Tg, low water absorption, low modulus, and excellent thermal stability

Product Description

LINQSOL EMC-7535 is a green epoxy molding compound specifically developed for high-voltage and high-power semiconductor devices. It offers low modulus to meet low-stress requirements. With a high glass transition temperature (Tg = 175 °C), minimal moisture absorption, a high comparative tracking index (CTI = 600 V), and a UL 94 V-0 flammability rating,  EMC-7535 guarantees strong performance and outstanding reliability.

Overall, LINQSOL EMC-7535 seamlessly integrates advanced material properties, safety compliance, and superior performance, precisely meeting the stringent demands of high-power semiconductor components such as TO packages.

Product Family

EMC-7535/18M13G15K

Pelletized - 18MM X 13GR | 15kg box
1. Select Package Type
2. Select Product Form
3. Select Pellet Size
4. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 16.5 kg
Dimensions 25 x 28 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
black
Filler Content
75 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.96
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
16000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.25 %
Physical Properties
Spiral Flow @ 175°C
86 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
175 °C
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Mechanical Properties
Molded Shrinkage
0.1 %
Curing Conditions
Transfer Pressure
40-90 kg/cm2
Transfer Time
10-25 s

Additional Information

Processing Instructions

  • Before use, let LINQSOL EMC-7535 reach room temperature for 24 hours. Keep the bag unopened and stored in a dry location with a relative humidity of ≤50% during thawing to prevent moisture contamination. 
  • Use the materials within 72 hours after removing the container from cold storage.

Storage and Handling

LINQSOL EMC-7535 is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life at 5 °C is 183 days.