LINQSOL EMC-7142 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LINQSOL EMC-7142 | Black Epoxy Mold Compound

Main features

  • Green epoxy molding compound
  • Designed for SOP and QFP
  • Low water absorption, low stress, and excellent moldability

Product Description

LINQSOL EMC-7142 is a green epoxy molding compound series specifically developed for the encapsulation of small outline packages (SOP) and quad flat packages (QFP). Its high spiral flow at 175 °C satisfying the required standards for SOP and QFP molding. LINQSOL EMC-7142 has low modulus that meets low-stress requirements. Additionally, with a UL 94 V-0 flammability rating and low water absorption.

EMC-7142 guarantees strong performance and outstanding reliability. This product is deliberately formulated without the inclusion of substances prohibited by the European Union RoHS and REACH. Previous packages using EMC-7142R met the MSL 1 preconditioning requirements successfully. Overall, LINQSOL EMC-7142 seamlessly integrates advanced material properties, safety compliance, and superior performance to deliver a reliable solution for semiconductor device encapsulation.

LINQSOL EMC-7142 series delivers robust performance and flexibility. Choose from standard (Type S) or low wire sweep (Type L) versions, both qualified in popular package options (SOP8, SOP14, SOP16) and meeting MSL3 requirements. With over 350 shots of moldability, these devices are designed for long-lasting reliability. Higher reliability variants (EMC-7142 and EMC-7142 Type H) are currently under development and evaluation.

Key Features

  • Good moldability performance.
  • Good flowability without wire sweep.
  • Good adhesion performance on Cu/Ag leadframe.
  • Good reliability performance on SOP package.
  • Low water absorption to meet MSL3 to MSL 1 requirements. 
  • Meets UL94 V-0 flammability. 
  • Green material without Br/Sb in compliance with ROHS.

Available Versions

  • EMC-7142 (Standard)
  • EMC-7142 Type L (Low Stress)
  • EMC-7142 Type R (MSL 1 Capable)
  • EMC-7142 Type H (High Voltage up to 900V Packages)

Reliability Tests Passed:

  • Preconditioning: Baking (125 °C for 24 hours) → Soak (30 °C, 60% RH for 192 hours → 3xReflow (260±5 °C)
  • PCT, Tₐ=121°C, P=2 atm, RH=100%* 168 hours
  • TCT, –65 to 150 °C * 500 cycles
  • HTST, T=150°C  * 1008 hours
Product Family

EMC-7142/14M4.3G15K

Pelletized - 14mm x 4.3gr | 15kg
1. Select Package Type
2. Select Product Form
3. Select Pellet Size
4. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 16.5 kg
Dimensions 25 x 28 x 26.5 cm

Technical Specifications

General Properties
Color
The color
Black
Filler Content
87 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.0
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
123 °C
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Chemical Properties
Water Absorption
0.3 %
Curing Conditions
Transfer Pressure
40–90 kg/cm2
Transfer Time
10–35 s
Physical Properties
Spiral Flow @ 175°C
116 cm

Additional Information

LINQSOL EMC 7142 Series Property Comparison

 
PROPERTY UNIT EMC-7142  EMC-7142L EMC-7142R EMC-7142H
Resin Type - MAR + Low Stress MAR MAR MAR + New
Filler Type - Spherical Spherical Spherical Spherical
Filler Content % 87 87 88 88
Specific Gravity  - 2.0 1.99 2.0 2.0
Spiral Flow @175°C cm 116 119.4 90 101.6
Hot Plate Gel Time @175°C sec 29 27 30 28
Glass Transition Temperature °C 123 127 122 128

CTE 1, α1

CTE 2, α2

ppm

ppm

8

38

9

37

8

34

8

37 

Flexural Strength @25°C

Flexural Modulus @25°C

MPa

Gpa

150

24.5

140

24

160

24.8

150

24

 Dielectric Strenght  KV/mm 13 13  14  14
Water Absorption % 0.15 0.3 0.18 0.26

Adhesion Strength at Cu substrate after Post Mold Cure
Adhesion Strength at Ni substrate after Post Mold Cure

Adhesion Strength at Cu substrate after MSL3 Preconditioning
Adhesion Strength at Ag substrate after MSL3 Preconditioning
Adhesion Strength at Ni substrate after MSL1 Preconditioning

MPa
MPa

MPa
MPa
MPa

-
0.465

4.61
4.12
-

-
0.422

5.32
4.15
MPa

7.7
2.62

4.58
4.15
1.27

-
2.53

4.58
5.9
1.39

Comments   STD/MSL3 Lower wire sweep MSL 1 High Voltage up to 900V MOS Packages
 

LINQSOL EMC-7142 Reliability Test Results for Small Outline Packages (SOP)

Device Information

Package Type 8SOP-225
Epoxy XXX1076XX
Leadframe 8SOP-225 (90 × 90); 8 × 32 SLF Cu
Wire 0.9 mm HS-RF2
Epoxy Mold Compound LINQSOL EMC-7142 (14 mm, 3.4 g)

 

Test Conditions

Test Item

Condition

Duration

Quantity

Pre-conditioning

Bake (125 °C)

Soak (30 °C, 60% RH)

Reflow (260±5 °C)

24 h

192 h

3 times

90 each

TCT

–65 to 150 °C

500 cycles

45 each

PCT

121 °C, 100% RH, 2 atm

96/168 h

45 each

HTS

150 °C

1008 h

45 each

 

Reflow Profile

Step

Profile Feature

Condition/ Duration

1

Minimum Temperature (Tsmin)
Maximum Temperature (Tsmax)
Time (ts) from Tsmin to Tsmax

150 °C
200 °C
60–120 s

2

Ramp-up Rate (TL to TP)

3 °C/s (maximum)

3

Liquidus Temperature (TL)
Time (tL) maintained above TL

217 °C
60–150 s

4

Peak Package Body Temperature (TP)

260±5 °C

5

Time (tp) within 5 °C of the Specified Classification Temperature (TC)

30 s

6

Ramp-down rate (TP to TL)

6 °C/s (maximum)

7

Time 25 °C to Peak Temperature

8 min maximum

 

Scanning Acoustic Tomography Results 

Test Item SAT Result (Fail Units/Total Units)
Test Result
  Top Chip Top Leadframe Pad Inner Lead  
Before 0/30 0/30 0/30 PASS
After MSL3 0/30 0/30 0/30 PASS

 

Scanning Acoustic Tomography Images

Test Item
Images
Pre-conditioning Before EMC7142SATReliabiltyImage_before
After EMC7142SATReliabiltyImage_after

 

Conclusion on EMC7142 Reliability Test Performance

All 8SOP-225 devices passed the reliability test without any failure. 

 

Test Item

In

Out

Yield

Test Result

Preconditioning

90

90

100%

PASS

TC (500 Cycles)

45

45

100%

PASS

PCT (96 h)

45

45

100%

PASS

PCT (168 h)

45

45

100%

PASS

HTS (1008 h)

45

45

100%

PASS

 

LINQSOL EMC-7142 Moldability Test Results

Beta Site (G) Performace of EMC-7142

Device Information

Package Type SOP8(12R)
Epoxy Mold Compound (EMC) EMC-7142
Die Size 0.56*0.405 mm
Die Thickness 300±20 μm
Pad Size 62*62 μm
Pad Pitch 80 μm
Lead Frame Silver Plated Copper
Wire 0.8mil/Cu20μm

 

Continuous Molding using EMC-7142 on SOP8

Molding Shot SAT Images Remarks
First mold MoldabilityofEMC-7142Shot#1 PASS
100th MoldabilityofEMC-7142Shot#100 PASS
150th MoldabilityofEMC-7142Shot#150 PASS
200th MoldabilityofEMC-7142Shot#200 PASS
250th MoldabilityofEMC-7142Shot#250 PASS
300th MoldabilityofEMC-7142Shot#300 PASS
330th MoldabilityofEMC-7142Shot#330 PASS
369th MoldabilityofEMC-7142Shot#369 PASS

 

Reliability Test Results after Continuous Molding using EMC-7142 on SOP8

Test Items Test Conditions SAT Images Results

Preconditioning MSL 3

+ 

TCT 200 cycles

SAT1
Bake: 125°C, 24h
Soak: 60°C, 60%RH, 40h
Reflow: 260°C, 3 times
TCT 200 cycles (-65~200°C)
SAT2
ReliabilityTestResults afterContinuousMoldingusingEMC-7142 on SOP8 PASS

 

Beta Site (S) Performace of EMC-7142

Package Type SOP8
Lead Frame Density 8 rows * 32 columns Lead Frame Type Cu with Ag-plating
Mold Type TOWA Y-1 Molding Temp (°C) 175
Preheat Time (sec) 3 T/F Pressure (ton) 1.3
Cure Pressure (ton) 55 T/F Time (sec) 10.2

 

Scanning Acoustic Tomography Results

No delamination after PMS/MSL3 

Test Item
Images
Pre-conditioning Before SATResultBeforePreconditioningonBetaSite(S)usingEMC7142
After SATResultafterPreconditioningonBetaSite(S)usingEMC7142

 

Wire Sweep Images

Spec  ≤15%

Left (1.5%) Center (2.2%) Right (1.6%)
EMC7142WireSweepPerformanceLeft EMC7142WireSweepPerformanceCenter EMC7142WireSweepPerformanceRight

 

Reliability Test Results on Site (S)

Test Item Condition Result
SAT MSL3
Bake(125°C) 24h,
Soak (30°C, 60%RH) 192h,
Reflow(260 +5/-0°C) 3 times
0/90
PCT 121°C, 100%RH, 2atm 0/45
TCT -65°C - 150°C, 500 cycles 0/45
HTS 150°C, 1008h 0/45

 

LINQSOL EMC-7142 Type L Moldability Test Results

Beta Site (C) Performace of EMC-7142 Type L

Device Information

Package Type SOP16
Lead Frame Density 12 rows * 20 columns Lead Frame Type Cu with Ag-plating
Wire 1.2 mil Molding Temp (°C) 175
Preheat Time (sec) 3 T/F Pressure (ton) 1.3
Cure Pressure (ton) 55 T/F Time (sec) 10.2

 

Scanning Acoustic Tomography Results using EMC-7142 Type L

No delamination after PMS/MSL3 

Test Item
Images
Pre-conditioning Before SATResultbeforePreconditioningonBetaSite(C)usingEMC7142TypeL
After SATResultafterPreconditioningonBetaSite(C)usingEMC7142TypeL

 

Wire Sweep Images using EMC-7142 Type L

Spec  ≤10%

Left (1.5%) Right (1.6%)
EMC7142TypeLWireSweepPerformance1 EMC7142TypeLWireSweepPerformance2

 

Beta Site (G) Performace of EMC-7142 Type L

Device Information

Package Type SOP14(12R)
EMC EMC-7142 Type L
Die Size 0.43*0.43 mm
Die Thickness 300±20 μm
Pad Size 62*62 μm
Lead Frame Silver Plated Copper
Wire 0.8mil/Cu20μm
Preconditioning MSL3 + TCT 200 cycles

 

Continuous Molding using EMC-7142 Type L  on SOP14

Molding Shot SAT Images Remarks
10th MoldabilityofEMC-7142TypeLShot#10 PASS
150th MoldabilityofEMC-7142TypeLShot#150 PASS
284th MoldabilityofEMC-7142TypeLShot#284 PASS
350th MoldabilityofEMC-7142TypeLShot#350 PASS

Reliability Test Results after Continuous Molding using EMC-7142 Type L on SOP14

Test Item Condition SAT Images Result

Preconditioning MSL 3

+

TCT 200 cycles

SAT 1

Bake: 125°C, 24h; 

Soak: 60°C, 60% RH, 40h;

Reflow: 260°C, 3 times

TC 200 cycles (-65°C to 200°C)
SAT 2

PASS

 

Processing Instructions

  • Before use, let LINQSOL EMC-7142 reach room temperature for 24 hours. Keep the bag unopened and stored in a dry location with a relative humidity of ≤50% during thawing to prevent moisture contamination. 

  • Use the materials within 72 hours after removing the container from cold storage.

Storage and Handling

LINQSOL EMC-7142 is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life when stored below 5 °C is 183 days.

Presentations

 

LINQSOL EMC-7142 Reliability Test Results

The presentation above shows the reliability performance of EMC-7142 evaluated using an 8SOP-225 package.

LINQSOL EMC-7142 Moldability Test Results

The presentation above shows the moldability performance of EMC-7142 evaluated using an SOP(12R) package. 

 

LINQSOL EMC-7142 Flammability Test Results

The presentation above shows the flammability test performance of EMC-7142R evaluated following UL94 Test Method. 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers