LINQCELL NFP 500 | Nickel Sintered Fiber Felt

Harmonization Code : 7508.10.00.00 | Cloth, grill and netting, of nickel wire

NFP 500 | Nickel Sintered Fiber Felt

Main features

  • 0.5mm - 500um - 19.6mil
  • Ni200 and Ni201 alloys
  • AEM and Alkaline Water Electrolysis

Product Description

LINQCELL NFP500 is a robust Nickel Fiber Felt with a thickness of 500μm, offered in both Ni200 and Ni201 alloys. Engineered with precision, this felt is produced in accordance with rigorous international standards, employing a meticulous felt laying process and high-temperature vacuum sintering.

LINQCELL NFP500 has a three-dimensional porous structure that is designed for optimal performance. Its elevated thickness, compared to NFP250, enhances its capacity for numerous applications where durability and efficiency are essential.

LINQCELL NFP500 offers exceptional corrosion resistance, a high specific surface area, and ensures outstanding longevity and reliability. Its uniform pore size distribution offers consistent performance across diverse applications.

Applications:

  • Filtration: NFP500 excels in applications requiring efficient separation and purification.

  • Air Quality: The increased thickness is particularly advantageous for air filter screens in applications like photocatalyst series air filters.

  • Catalyst: Its uniform pore size distribution is invaluable for chemical catalysis processes, aiding in reactions and efficiency.

  • Batteries: NFP500, with its thicker profile, is an ideal choice for electrode materials, extending the life of batteries.

  • Heat Control: The increased thickness offers heightened heat dissipation capabilities, making it perfect for applications with demanding temperature control needs.

LINQCELL NFP500, with its enhanced thickness, provides an even more robust solution for applications requiring durability and efficiency. Its technical attributes and benefits make it an indispensable component in various industries, ensuring enduring performance in challenging conditions.

Product Family

NFP500/200NI20X20

Alloy: Ni200 - 20x20cm
1. Select Sheet Size
2. Select Alloy Type

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Unit of measure Sheet
Net weight 0.007 kg
Gross weight 0.0077 kg
Dimensions 20 x 20 x 0.05 cm

Technical Specifications

General Properties
Porosity
Void fraction is a measure of the void spaces in a material
50-90 %
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
500 μm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
≥8 %

Leading Brands Trust in Our Products and Services