LINQCELL NFP 250 | Nickel Sintered Fiber Felt

Harmonization Code : 7508.10.00.00 | Cloth, grill and netting, of nickel wire

NFP 250 | Nickel Sintered Fiber Felt

Main features

  • 0.25mm - 250um - 9.8mil
  • Ni200 and Ni201 alloys
  • Excellent catalyst support

Product Description

LINQCELL NFP250 is a versatile 250μm Nickel Fiber Felt, available in Ni200 and Ni201 alloys. It is engineered in compliance with international standards, using a precision felt laying process and high-temperature vacuum sintering. Nickel materials are commonly used in AEM and Alkaline Water Electrolysis.

LINQCELL NFP250 features a unique three-dimensional porous structure, setting it apart from conventional nickel materials. Its high porosity and specific surface area ensure efficient permeation and diffusion, making it ideal for diverse applications. The uniform pore size distribution guarantees consistent performance. Crafted from high-quality Ni200 and Ni201 alloys, LINQCELL NFP250 boasts impressive corrosion resistance, promising longevity and reliability. Its excellent water permeability and heat dissipation properties add to its suitability for various applications.

Applications include:

  • Catalyst Support: The uniform pore size distribution and large surface area are valuable in chemical catalysis processes.

  • Battery Technology: Enhance electrode performance and lifespan with LINQCELL NFP250 as a battery electrode material.

  • Filtration: LINQCELL NFP250's high porosity and structure make it perfect for effective separation and purification in filtration applications.
  • Air Purification: Ideal for air filter screens where air quality is a priority, especially in photocatalyst series applications.

  • Heat Exchange: Its heat dissipation properties make it an excellent choice for applications that require temperature control.

LINQCELL NFP250 is a dependable and practical solution for a wide range of applications. Its technical properties and benefits make it an essential component in various industries, ensuring efficient performance and lasting durability in challenging conditions.

Product Family

NFP250/200NI20X20

Alloy: Ni200 - 20x20cm
1. Select Sheet Size
2. Select Alloy Type

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Unit of measure Sheet
Net weight 0.0035 kg
Gross weight 0.0039 kg
Dimensions 20 x 20 x 0.025 cm

Technical Specifications

General Properties
Porosity
Void fraction is a measure of the void spaces in a material
40-90 %
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
250 μm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
≥8 %

Additional Information

Key Features:

  • Three-Dimensional Porous Structure: LINQCELL NFP250 boasts a remarkable three-dimensional network porous structure, setting it apart from conventional nickel mesh or nickel powder sintered plates.

  • High Porosity: With porosity levels optimized to perfection, this nickel fiber felt allows for efficient permeation and diffusion, making it an ideal choice for various applications.

  • Large Specific Surface Area: Thanks to its unique construction, LINQCELL NFP250 offers a substantial specific surface area, providing excellent contact points for your specific needs.

  • Uniform Pore Size Distribution: The precisely engineered uniform pore size distribution ensures consistent performance across the material, leading to reliable results every time.

  • Corrosion Resistance: Crafted from high-grade nickel alloys (Ni200 and Ni201), our fiber felt exhibits robust corrosion resistance, ensuring long-lasting durability.

  • Water Permeability: Enjoy the advantages of good water permeability, allowing for effective and efficient use in various applications.

  • Exceptional Heat Dissipation: LINQCELL NFP250 excels in heat dissipation, making it a preferred choice in applications where temperature control is paramount.

  • Stability and Longevity: Designed to meet stringent quality standards, this product promises stability, long life, and dependable performance in demanding conditions.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers