LINQCELL GDL1000 | 1.0mm Carbon Plate

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

LINQCELL GDL1000 | 1.0mm Carbon Plate

Main features

  • 1.00 mm – 1000 µm – 39 mil
  • High electrical conductivity and tunable compressibility
  • Porous transport and gas diffusion layers for water electrolyzers and fuel cells

Product Description

LINQCELL GDL1000 is a 1.00-mm thick graphitized carbon fiber paper made from high-quality polyacrylonitrile (PAN) fibers. These fibers undergo a wet-laying paper process using a specially formulated carbonizable resin, resulting in a non-woven, fibrous, and porous structure, which is then carbonized and graphitized for enhanced performance. GDL1000 exhibits high electrical conductivity due to high-temperature treatment above 1000 °C, good oxidation resistance, and excellent thermal stability.

Key Features:

  • Low electrical resistance (TP Resistance = 11.11 mΩ⋅cm2)
  • High porosity
  • Good oxidation resistance
  • Excellent thermal stability 

     

These characteristics make LINQCELL GDL1000 highly recommended for use as cathode porous transport layers in PEM and/or AEM water electrolyzers, as well as gas diffusion layers in fuel cells. 

Highly Recommended for:

LINQCELL GDL1000 is graphitized at 1600 °C but can also be produced at a higher graphitization temperature (2000 °C) to meet high-performance device requirements. Higher graphitization results in better electrical performance while significantly increasing the material cost. It is mainly recommended when resistivity is of the utmost importance.

Product Family

GDL1000/20X20

200 x 200mm Sheet
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Sheet
Net weight 0.0232 kg
Gross weight 0.025 kg
Dimensions 20 x 20 x 0.1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
580 g/m2
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
1000 μm
Electrical Properties
Through Plane Resistivity
Resistance of the amount of current through a material
109.86 mΩcm
TP Resistance
Opposition to the flow of electric current.
11.11 mΩcm2
Voltage loss
25.20 mV