Main features

  • 0.4mm - 400um - 16mil
  • Comes in roll form
  • 13 TP Resistance

Product Description

LINQCELL CF400-MP is a 0.4mm thick carbon cloth with a Microporous layer and PTFE. It is commonly used as a gas diffusion layer and electrode for fuel cells. Its through-plane resistivity is less than 13 mΩcm2.

LINQCELL CF400-MP is typically used in PEM fuel cells as well as PA and DM fuel cell applications as a gas diffusion layer. These thinner gas diffusion layers offer good electrochemical performance and can also lend themselves to AEMFC GDL Anodes. Thickness has more sensitivity to the AEMFC when used in the anode electrode rather than in the cathode electrode, indicating that water removal at the anode was more challenging than water supply at the cathode so the strategy of water management among electrodes should be differentiated.

Carbon cloth based GDLs have performance equal to that of conventional carbon papers. Carbon cloth is more practical than carbon paper because of its superior compressibility, elasticity, and flexibility performance, making it more appropriate for ongoing manufacturing and assembly processes. Carbon cloths with a Microporous layer can achieve the required performance and provide an alternative option to carbon paper as GDL. Standard LINQCELL CF400-MP contains 10 wt% PTFE wet-proofing, and the PTFE content can be customized based on your specific requirements.

 

Product Family

CF400-MP/M2

50cm x 200cm | Roll form
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Roll
Net weight 0.64 kg
Gross weight 0.704 kg
Dimensions 200 x 50 x 0.04 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
200 g/m2
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
410 μm
Electrical Properties
TP Resistance
Opposition to the flow of electric current.
13 mΩcm2
Mechanical Properties
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
10 N/cm