XVCF-3S500 | LINQSTAT 3 mil - 500 Ω/sq Conductive Film

Harmonization Code : 3920.10.28.99 | Polymers of Ethylene Plates, Sheets, Film, Foil, Tape, or Strips (Non-cellular), having a thickness not exceeding 0.125mm, having a specific gravity of 0.94 or more

LINQSTAT XVCF - Carbon Electrodes XVCF-3S500 | LINQSTAT 3 mil - 500 Ω/sq Conductive Film LINQSTAT XVCF 500 Ohms/sq 3 mil Conductive Film

Main features

  • 3 mil - 76um - 0.07mm
  • ±500 ohms/sq Surface resistivity
  • ±3.5 ohms-cm Volume resistivity

Product Description

LINQSTAT™ XVCF-3S500 is a highly conductive conductive polyethylene film similar to our standard VCF-Series film but with a higher electrically conductive carbon loading and a denser polymer mix. Having a surface resistance of ±500 ohms/sq, this extra loading makes the XVCF-Series more conductive than our standard film and allows it to be used in applications that require a lower resistivity. In addition, the film is volume conductive, claiming a mere 3.5 ohms-cm volume resistivity.

LINQSTAT™ XVCF-3S500 conductive films are thin (0.07mm or 3 mil), lightweight and relatively inert. Furthermore, they are well suited for applications requiring electrochemical reactions, high conductivity or charge storage including but not limited to electrodes (ECG, TENS, Defibrillation and Iontophoresis), batteries (flat-cell zinc/manganese dioxide (MnO2), Lithium Ion and Lithium polymer), wearable electronics and digital whiteboards.

LINQSTAT™ XVCF-3S500 film and its conductivity are unaffected by humidity and age. The film is heat sealable, flexible and offers exceptional abrasion resistance. The film gives good thermal stability and has outstanding chemical resistance. It has a standard thickness of 76µm (3 mil) and is available in various lengths and widths upon request. The standard core size is 3" but some widths are also available with a 6" core.

Product Family

XVCF-3S500/30CM-46M

30cm wide x 46m long
1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Roll
Net weight 1.06 kg
Gross weight 1.66 kg
Dimensions 30 x 13 x 13 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Carbon-Loaded PE
Color
The color
Black
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
0.07 mm
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.10
Electrical Properties
Surface Resistivity
500 Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
3.5 Ohms⋅cm
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes

Additional Information

Heat sealing

  • Heat sealing time: 0.5-3.5 sec
  • Heat sealing pressure: 30-70 psi
  • Heat sealing temperature: 135 °C - 190°C 

 

Given its low surface resistance, LINQSTAT XVCF films have been successfully used as a pressure sensor making them useful for applications that require more conductivity to be able to detect more subtle pressure differences.

Applications:

  • ECG electrodes
  • TENS electrodes
  • Defibrillation electrodes
  • Digital white boards
  • Lithium ion / polymer battery
  • Flat-cell MnO2 battery

Due to its low-resistivity and its resistance to a range of chemicals and alcohols, these films are suitable for use in electrodes. Their matte finish allows them to be printed on, and the low material thickness makes them flexible to adapt well to a range of contours.

Chemical Susceptibility:

  • Methanol: Resistant
  • Ethanol: Resistant
  • Isopropanol: Resistant
  • Weak Acids: Resistant
  • Ketones (Acetone): Slow Attack
  • Weak Alkalines: Slow Attack
  • Hydrocarbons: Non-Resistant

Product Features & Benefits:

  • Volume-conductive plastic
  • Black Opaque - Printable
  • Provides Anti-Static protection to electronics components
  • Groundable
  • Humidity independent conductivity
  • Thin, Lightweight, Inert 

We have recently changed our SKUS. To help you search for them either on google or on our website here's a before and after table. As you can see we went for the "Product codes that make sense" approach:

XVCF-30009BT500S/9 XVCF-3S500/23.8CM-1524M 23.8cm wide x 1524m long
XVCF-30009BT500S/2 XVCF-3S500/23.8CM-46M 23.8cm wide x 46m long
XVCF-30012BT500S/2A XVCF-3S500/30CM-46M 30cm wide x 46m long
XVCF-30012BT500S/4A XVCF-3S500/30CM-500M 30cm wide x 500m long

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers