WS830 | Wax Conditioning Sheets

Harmonization Code : 4005.91.00.00 | Compounded rubber, unvulcanized, in primary forms or in plates, sheets or strip: Plates, sheets, and strip

WS830 | Wax Conditioning Sheets

Main features

  • High flow
  • Excellent elastic properties
  • Homogeneous waxing

Product Description

CHEMLINQ WS830 Wax Conditioning Sheets are used to protect the mold surface and ensure a good releasing effect after cleaning. It is a waxing sheet that provides an ideal balance between great mold protection and high workability and it can be used for Green and non Green EMC as well as manual and auto molding processes.

CHEMLINQ WS830 performs well in a wide range of molds and has a curing time of ~ 180-240 seconds. These sheets are highly effective as a protection and release product. They have good flow characteristics which enable them to easily reach into the mold corners and thin gate areas. Used in combination with our RCS Rubber Cleaning Sheets, the short mold waxing and cleaning time will lead to reduced costs and will increase your overall efficiency and productivity.

Product Key Features

  • High Flow — decreases friction, thus making the molding cycle faster and more efficient..
  • Homogenous Waxing — improves lubrication; ensures efficient and even coverage of the mold surface

Applications

  • Improving mold release during semiconductor molding process

 

Product Family

WS830/23T5S15K10

10 kg | 230mm x 5mm x 15mm (Slot)
1. Select Width
2. Select Length
3. Select Thickness
4. Select Slot Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 10.5 kg
Dimensions 23 x 10 x 0.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
grey
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1 - 1.3
Other Properties
Shots
1-2

Additional Information

Compatible Working Conditions

Clamp pressure 1600 – 1800 psi or 
50 – 120 tons
Mold temperature ±175°C
Curing time 180-250 Seconds
#of shots 1-2 Shots

Usage

  • Place 1-2 WS830 strips per mold chase depending on the frame and mold cavity design.
  • Clamp the mold to fully fill up all the mold cavities.
  • Over clamping the compound may cause releasing difficulties from mold.
  • The suggested compound cure time is dependent on mold temperature.
  • For normal molding temperatures of 175 ±5 °C, the cure time ranges from 180 to 240 sec.
  • The number of conditioning shots suggested is 1 to 2 shots after mold cleaning.
  • Curing the product for more than 10 mins for 180 °C might create sticking problems.

 

Storage and packaging

The wax conditioning and release sheets come in one size that will fit a variety of molds, so you can use one waxing product for all your molds. Other dimensions are possible after customer request and are subject to MOQ. 

CHEMLINQ conditioning sheets come prepackaged in PE bags and in 10Kg carton boxes. They need to be stored and transferred in a cool environment and their work life is 4 days after removal from the storage conditions.

Shelf life is 9 months from the manufacturing date if stored in a cool, dry, air-conditioned room.