WS800 | Wax Conditioning Sheets

Harmonization Code : 4005.91.00.00 | Compounded rubber, unvulcanized, in primary forms or in plates, sheets or strip: Plates, sheets, and strip

WS800 | Wax Conditioning Sheets

Main features

  • Excellent conditioning for green EMCs
  • Fast cure time
  • No lead frame and preheating required

Product Description

CHEMLINQ WS800 is a specially formulated wetting and conditioning compound designed for use after the cleaning cycle of thermosetting transfer molds. This advanced compound is compatible with RCS series rubber cleaning materials. WS800 offers conditioning properties with minimal application shots, resulting in reliable mold performance without solderability issues or over-waxing of mold cavities. Its fast-curing formulation significantly reduces cure time, improving productivity and efficiency in mold conditioning. CHEMLINQ WS800 does not require preheating and lead frames during the conditioning process. The compound ensures a good release from the mold after curing, further shortening the time required for mold conditioning.

Product Family

WS800/23T5S10K10

10 kg | 230mm x 5mm x 10mm (Slot)
1. Select Width
2. Select Length
3. Select Thickness
4. Select Slot Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 10.2 kg
Dimensions 23 x 10 x 5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Pink-Red Solid Strips
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1 - 1.3

Additional Information

WS800 Additional Specifications

Property Value
pH Neutral to mild alkaline
Solubility Insoluble in water

Instructions for Use

  • Place strips on the mold chase. Strip quantity depends on the mold dimension.

  • Clamp the mold and compress to fill all the cavities carefully, as overclamping may cause releasing difficulty from the mold.

  • Recommended cure time for 175 + 5 °C is 2–5 minutes. Cure time depends on the mold temperature.

  • Avoid overcuring, i.e., curing at 175 °C for 10 minutes,  because it may cause the material to stick to the mold.
  • Repeat until you achieve the required conditioning result.

 