TMC-8020LS | Clear Optical Molding Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

TMC-8020LS | Clear Optical Molding Compound

Main features

  • LED Encapsulation
  • Low stress
  • Better reflow and Thermal shock

Product Description

OPTOLINQ TMC-8020-LS is a high-performance optical solid epoxy specifically developed for LED encapsulation. This monocomponent epoxy achieves superior adhesion performance and great transmittance. It has lower Tg than the "normal" 8020 version.

OPTOLINQ TMC-8020-LS is able to offer low blue-ray decay for outdoor LED applications and overall great light performance. This low stress white epoxy is very close to competitive solutions such as XX814, XX1000 and XX97. It is a reliable product that has improved reflow abilities and thermal shock test performance.

Product Family

TC8020LS/35M25G10K

35mm x 25GR - 450nm transmittance | 10 Kg Box
1. Select Package Type
2. Select Pellet Size
3. Select Pellet Weight
4. Select Transmittance

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 11 kg
Dimensions 25 x 25 x 25 cm

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Blue Tablet
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.2
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
95 °C
Chemical Properties
Water Absorption
0.17 %
Curing Conditions
Transfer Pressure
10 - 40 kg/cm2
Transfer Time
20 - 50 s
Physical Properties
Spiral Flow @ 175°C
150 - 250 cm

Additional Information

 
 TMC-8020 Low Stress Products Properties Comparison
 
PROPERTY UNIT TMC-8020L TMC-8020LS
Viscosity  cP 300 200
Spiral Flow @150°C cm 150-250 150-250
Hot Plate Gel Time @150°C sec 25-50 20-50
Glass Transition Temperature °C 115 95

CTE by TMA, α1

CTE by TMA, α2

ppm

ppm

70

170

70

220

Moisture Absorption PCT

24 hrs @25°C water

24 hrs @121°C, 2atm, 100%RH

 

wt%

wt%

 

0.16

3.2

 

0.17

3.8

Flexural Strength @25°C

Flexural Modulus @25°C

MPa

Mpa

130

2900

110

3100

yellowing Δb - 4 hrs @200°C

yellowing Δb - 30 min @280°C

yellowing Δb - 4 hrs UV

-

8

42

16.5

25

45

16.5

Transmittance 1mm @450nm % >90 >90
Refractive Index @633nm - 1.56 1.56
Comment   Low stress version for better reflow performance Low stress for balanced reflow and thermal shock test performance
 