SACQ | Pb-free Solder Spheres

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

SACQ | Pb-free Solder Spheres

Main features

  • Leadfree Solder Spheres
  • Excellent Solder Joint Reliability for small devices
  • Excellent fatigue resistance

Product Description

LINQALLOY SACQ solder spheres are lead free Tin/Silver/Copper/Bismuth/Nickel alloys that contain 92.45% Tin (Sn), 4% Silver (Ag),0.5% Copper (Cu), 3% Bismuth (Bi), and 0.05% Nickel (Ni).

LINQALLOY SACQ solder spheres offer higher reliability than SAC405, in small, and thin devices, particularly in WLCSP and WLFO designs.

Features:

  • Excellent Fatigue Resistance
  • Compatible with all Flux Types
  • Excellent Solder Joint Reliability
  • Best Wetting Sn/Ag/Cu/Bi/Ni Alloy

Each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder spheres and ensures the SAC405 solder spheres meet the following quality criteria:

  • Tin (Sn): 92.45%
  • Silver (Ag): 4%
  • Copper (Cu): 0.5%
  • Bismuth (Bi): 3%
  • Nickel (Ni): 0.05%
  • Melting Temperature (Solidus): 211°C
  • Melting Temperature (Liquidus): 216°C
  • Sphericity: Within 1.5%

Diameter Tolerance

  • 0.22mm - 0.48mm (220µm - 480µm) : ± 0.010mm (± 10µm)
  • 0.50mm - 0.762mm (500µm - 762µm) : ± 0.025mm (± 25µm)

Product Family

SACQ/0.300-250kpcs

Alloy: Sn92.45/Ag4.0/Cu0.5/Bi3.0/Ni0.05 » 0.300mm (12mil) » 250,000 spheres
1. Select Diameter
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Jar
Net weight 0.0267 kg
Gross weight 0.0294 kg
Dimensions 6 x 6 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes
General Properties
Alloy Composition
Composition of the alloy material
Sn92.45Ag4Cu0.5Bi3.0Ni0.05
Alloy Type
A metallic element type
SACQ
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
7.56g/cc

Additional Information

What do I get when I buy SACQ Solder Spheres from KRAYDEN?

The advantage of ordering solder spheres online at KRAYDEN.com is that you can be sure of the quality. The solder spheres you receive are originally manufactured solder spheres packed into jars with inert gas (nitrogen). We do not repack the solder balls we receive, so the jars you will receive have never been opened, thus ensuring the quality of the product you receive. The lid of the jar is also always sealed with a shrink-wrapped plastic wrap ensuring that the solder spheres do not oxidate in the jar.

Presentation

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers