RCS 880 | Rubber Cleaning Sheets

Harmonization Code : 4005.91.00.00 | Compounded rubber, unvulcanized, in primary forms or in plates, sheets or strip: Plates, sheets, and strip

RCS 880 | Rubber Cleaning Sheets

Main features

  • Great releasing properties
  • No leadframe required
  • Excellent for vents and cavities

Product Description

RCS 880 Rubber cleaning sheets are used to eliminate pollutants and stains formed on the mold surface. They perform well in a wide range of molds and are able to withstand up to 100t. These sheets offer an good cleaning performance with less smell and fumes. 

RCS 880 sheets have good flow characteristics which enable them to clean mold corners and thin gate areas easily. Unlike melamine cleaners, RCS cleaning sheets can even clean the air ventilation areas without causing mold abrasion or corrosion. At the same time there's no need for dummy lead frame or preheating, something that reduces cleaning time and leads to improved production time results and productivity. 

RCS 880 Rubber cleaning sheets can remove contamination of molds used in the semiconductor industry for products such as as integrated circuits, diodes, transistors, and LEDs in both physical and chemical mechanisms.

Product Family

RCS880/23T5S10

10 kg | 230mm x 5mm x 10mm (Slot)
1. Select Length
2. Select Thickness
3. Select Slot Size

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 10.5 kg
Dimensions 35 x 25 x 20 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
White
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.2
Other Properties
Shots
3-6

Additional Information

Difference between RCS 620 and RCS 880

RCS 880 have higher elastomer content (55%) compared to RCS 620 (40-50%) which makes it more flexible/elastic thus enabling it to reach corners and complex portions of the mold while cleaning.

In addition, RCS 880 has more concentrated cleaning ability since it has no solvent in the composition while RCS620 have additional propylene glycol compound that act as a solvent/plasticiser.

 

 

Recommended Application Setting

RCS 620 & 880

Mold Pressure

1600 – 1800 psi or 

50 – 120 tons

Mold Temperature

150 – 185 ° degree celcius 

Curing Time

150 – 600 seconds

No of Shots

4 to 8 shots

 

Storage and packaging

These rubber sheets should be kept in room temperature. Their shelf life in these storage conditions is 9months.

They are packaged in PE bags and come in 10Kg (net) boxes. Exact width is not stated since the sheets can be arrayed for the application and width is adjusted to the box size to accommodate the net weight.

 

Sheet dimensions

  Sizes (in mm) Tolerances (in mm)
Length 230 ±5
Width 15 ±2
Thickness 5 ±1

 

Warning

It is recommended to use the sheets in a well ventilated area. Your skin should not come in contact with them when the rubber is hot and you should avoid storing them at temperatures above 30°C.