MCN-T20 | Transfer-Grade Wax Conditioning Pellets

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MCN-T20 | Wax Conditioning Pellet

Main features

  • Wax Compound
  • Filling deep cavities
  • Transfer Molding

Product Description

MCN T20 is a Wax conditioning compound that can be applied via transfer molding. The continuous molding and curing of molding compounds accumulates residues on the metal surface of the mold, making it lose its release ability and causing the surface quality to decay as a result. It is an amazing solution for those that don't want to stop the production process at all. You clean with a few shots of transfer cleaning compounds, you condition with MCN T20 and you keep your production running literally 24/7.

MCN T20 Wax compound has good workability with minimal odor and exceptional fluidity. It is able to easily fill deep cavities with excellent wax emitting that spreads a thin and lasting layer of releasing agent  to help recover the release ability of the mold.

Product Family

MCN-T20/B49E7.6

Pelletized - 14MM x 7.6GR | 10kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 10.51 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Gray Tablet
Filler Size Cut
75 µm
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.90
Curing Conditions
Transfer Pressure
90-110 Kg/mm2
Transfer Time
5-10 s
Physical Properties
Spiral Flow @ 175°C
152 cm

Additional Information

Where does this fit in the cleaning and conditioning process?

Conditioning with wax compounds or sheets are the two final steps of the cleaning process.

  1. Remove mold stains, and recover the cleanliness of mold die surface 
  2. Decompose mold stains, by the effects of dissolving, wrapping and grinding 
  3. Reduce the adhesion of mold stain to metal surface, by cleaning agents
  4. Wrap and remove mold stains by polymer cross linking at high temperature Cleaning
  5. Recover the release ability of mold die for molding compounds
  6. Spread a thin and lasting layer of releasing agent (wax)

MCN T20 Hardness Condition at Varying Mold Temperature

MCN T20 Hardness Condition at Different Mold Temperature

MCN T20 Gel Time & Spiral Flow Trend at Storage Condition 30°C | 30% RH

MCN T20 Gel Time & Spiral Flow Trend at Storage Condition 30°C | 30% RH

 

 

Note: : Spiral flow is expressed as the percentage of initial value.

 

Manufacturing capabilities

 

Product specifications (pellet size and weight) Appearance Diameter (mm) Weight (gr) Height (mm)
13*3.5 Grey 13 3.3~3.7 13~15.0
13*4.0 Grey 13 3.8~4.2 15.4~17.0
13*4.5 Grey 13 4.5~4.8 18.2~20.0
13*5.0 Grey 13 4.8~5.2 19.7~22.9
14*4.5 Grey 14 4.3~4.7 15.4~17.0
14*5.0 Grey 14 4.8~5.2 16.8~18.4
14*5.5 Grey 14 5.3~5.7 18.8~20.0
14*5.9 Grey 14 5.7~6.1 20.1~21.7
14*6.5 Grey 14 6.3~6.7 22.0~23.6
14*7.0 Grey 14 6.8~7.2 23.8~25.4
14*7.6 Grey 14 7.4~7.8 26.1~27.7
16*6.5 Grey 16 6.3~6.7 17.0~18.6
16*7.0 Grey 16 6.8~7.2 18.1~19.7
16*8.0 Grey 16 7.8~8.2 21.2~22.8
16*8.2 Grey 16 8.0~8.4 21.7~23.3
16*8.6 Grey 16 8.4~8.8 23.0~24.6
16*9.0 Grey 16 8.8~9.2 23.7~25.3
16*10 Grey 16 9.7~10.3 26.9~28.5
16*11 Grey 16 10.0~11.0 28.9.30.5
18*10 Grey 18 10.2~10.5 ~23.3
18*12 Grey 18 11.7~12.3 25.5~27.1
18*12.4 Grey 18 12.2~12.8 26.0~27.6
18*14 Grey 18 13.7~14.3 29.8~31.4

 