MCL-T20 | Melamine Transfer Cleaning Pellets

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MCL-T20 | Melamine Transfer Cleaning Pellets

Main features

  • Excellent Cleaning Efficiency
  • Ideal for High-Precision Industries (Electronics and Automotive)
  • Enhanced Mold Lifespan and Minimized Downtime

Product Description

CHEMLINQ MCL T20 is a mold cleaning compound tablet composed of melamine resin, silica filler, and other additives. The material is designed for the meticulous cleaning of metal mold dies in transfer molding processes. It effectively removes organic and inorganic residues and stains from mold dies used in transfer molding. Moreover, MCL T20 revitalizes mold surfaces, ensuring optimal performance and prolonging the operational lifespan of molds. Ideal for industries requiring precision and reliability in molding processes.

CHEMLINQ MCL T20 can be used alone or partnered with cleaning rubber sheets to enhance cleaning performance. 

Product Key Features

  • Effective Residue Removal — Meticulously cleans metal mold dies, eliminating both organic and inorganic residues and stains, prolonging the lifespan of metal molds..
  • Can be used in conjunction with cleaning rubber sheets for improved cleaning effectiveness.

Applications

  • Cleaning metal molds for transfer molding processes.
Product Family

MCL-T20/14M5G10K

10Kg - 14mm x 5gr

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
White
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.60
Physical Properties
Spiral Flow @ 175°C
55.9 cm

Additional Information

Recommended molding parameters
Mold Condition Conventional Auto Unit
Mold temperature 160-190 160-190 ℃
Preheating - 0-10 sec
90-110 - ℃
Transfer pressure 30-140 90-110 kgf/cm2
Transfer time 20-40 8-25 sec
Curing time 5-15 4-10 min

 

Preparation Instructions

1. Ensure the mold temperature is appropriate for cleaning, typically around the operating temperature of the mold. Make sure the mold is free from any significant debris or loose contaminants. 
2. Place the MCL-T20 tablets into the mold cavity. The number of tablets depends on the size of the mold and the level of contamination.
3. Close the mold and initiate a standard transfer molding cycle. This includes applying the necessary pressure and heat to activate the cleaning compound. The heat and pressure help the MCL-T20 tablets to flow across the mold surfaces, effectively loosening and removing organic and inorganic residues.
4. After the cycle is complete, open the mold and eject the cleaning compound residue. Inspect the mold for any remaining contaminants. If necessary, repeat the process using additional tablets or in combination with other cleaning methods, such as CHEMLINQ RCS rubber cleaning sheets.
5. Perform a final inspection to ensure all residues are removed.

Storage and Handling

1. The cleaning compound is sealed in PE bags, with 10 kg per carton.
2. Ensure the product stays dry, as high humidity can cause curing failures in the cleaning compound. Keep the product away from heat sources, as excessive heat can make the cleaning compounds ineffective.
3. Store the product below 25 °C. If taken from a cold room or refrigerator, thaw it in the sealed package for 18 to 24 hours until it reaches room temperature.
4. The shelf life is 6 months if stored at temperatures ≤ 25 °C and 12 months at temperatures ≤10 °C.