Main features

  • 95 µm film thickness
  • UV removable acrylic adhesive
  • Strong adhesion for silicon wafer applications

Product Description

LINQTAPE™ DCT-PVC95 is a polymerized vinyl chloride tape used in the dicing process. It provides an excellent balance of electrical, mechanical, thermal, and chemical properties. Its strong adhesion ensures the wafer remains secure during different manufacturing processes like die-cutting.  The security the tape provides prevents wafer damage, whiskers, soaking and allows for cleaner cuts. 

LINQTAPE™ DCT-PVC95 can be peeled by using UV. To ensure a clean substrate after removing the tape, DCT-PVC95 utilizes a technology through which after applying UV light, the adhesive (3,200 N/25mm) becomes less tacky (140 N/25mm), which facilitates the removal of the tape. This quality makes the tape ideal for glass, sensitive substrates, and applications for which the final product must be clean of any residue. DCT-PVC95 is a translucent 80µm film, with a one-sided 15µm acrylic adhesive layer, and backed with a PET liner. It is ideal for small chips. 

Key Features

  • Strong adhesion to prevent wafer damage
  • UV removable adhesive
  • No residue
  • Can be used with uneven surfaces
  • Antistatic
  • High Transparency
  • High and evenly distributed elasticity 
  • High heat tolerance (60 °C for a few minutes)

Application Ideas

  • Die -cutting
  • Glass and sensitive applications 
Product Family

DCT-PVC95/300

300mm (11.8") wide x 100m (109yd) long

Loading pricing…

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Acrylic
Adhesive Thickness
Adhesive thickness indicates the thickness of an adhesive layer. It refers to the adhesive thickness of a single side so for double sided tapes it always needs to be multiplied.
15 µm
Appearance
Appearance at room temperature.
Translucent
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
80 µm
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
PET
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
95 μm
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
10790 Oz/in
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
320 lengthwise, 340 crosswise %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
31 lengthwise, 25 crosswise N/cm