DCT-PO200 | Polyolefin Dicing Tape

Harmonization Code : 3920.10.89.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials; Of polymers of ethylene; Of a thickness exceeding 0,125 mm; Other; Other; Other

DCT-PO200 | Polyolefine Die Cutting Tape

Main features

  • 200 µm film thickness
  • UV removable acrylic adhesive
  • Gentle adhesion for packaging substrates and glass

Product Description

LINQTAPE™ DCT-PO200 is a frosted polyolefin (PO) tape used in the dicing process. It provides an excellent balance of electrical, mechanical, thermal, and chemical properties. Compared to a PET dicing tape, PO dicing tapes have the same strong adhesion but are more easily removed from the substrate. This makes it ideal for applications such as packaging substrates, or delicate substrates where gentler adhesion is required for easier removal. DCT-PO200 is a higher viscosity formulation compared to DCT-165, providing the tape with higher moisture, heat, and environmental resistance. Higher viscosity also increases the adhesion strength of the tape. 

LINQTAPE™ DCT-PO200 can be peeled by using UV. To ensure a clean substrate after removing the tape, DCT-PO200 utilizes a technology through which after applying UV light, the adhesive (23,000 N/25mm) becomes less tacky (200 N/25mm), which facilitates the removal of the tape. This quality makes the tape ideal for glass, sensitive substrates, and applications for which the final product must be clean of any residue. DCT-PO200 is a 150µm PO film, with a one-sided 50µm acrylic adhesive layer, and backed with a PET liner. This product can be customized according to the customer's needs. 

 

Key Features

  • Strong adhesion to prevent substrate damage
  • Can be used with uneven surfaces
  • Antistatic
  • High transparency
  • High flexibility
  • High chemical resistance 
  • No residue after removal

Application Ideas

  • Masking
  • Temporary bonding
  • Assembly of delicate components
  • Packaging substrates
  • Glass (e.g. optical applications)
Product Family

DCT-PO200/300

300mm (11.8") wide x 100m (109yd) long

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Acrylic
Adhesive Thickness
Adhesive thickness indicates the thickness of an adhesive layer. It refers to the adhesive thickness of a single side so for double sided tapes it always needs to be multiplied.
50 µm
Appearance
Appearance at room temperature.
Frosted
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
150 µm
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
PET
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
200 μm
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
82735 Oz/in
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
903 lengthwise, 867 crosswise %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
34 lengthwise, 31 crosswise N/cm