BGT-PO180 | Polyolefin Back Grinding Tape

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

BGT-PO180 | Polyolefine Back Grinding Tape

Main features

  • 180 µm film thickness
  • Urethane UV removable adhesive
  • High accuracy and easy to peel

Product Description

LINQTAPE™ BGT-PO180 is a translucent polyolefin (PO) tape used in the wafer back grinding process. It is compatible to the BG standard, and is highly accurate. The tape provides an excellent balance of electrical, mechanical, thermal, and chemical properties. PO tapes have the same strong adhesion as a PET tape but are more easily removed from the substrate. This makes it ideal for applications where easy removal without any residue left behind is required. BGT-PO180 is has a low-viscosity adhesive, and is resistant to warpage. 

LINQTAPE™ BGT-PO180 can be peeled by using UV. To ensure a clean substrate after removing the tape, BGT-PO180 utilizes a technology through which after applying UV light, the adhesive (18,000 N/25mm) becomes less tacky (80 N/25mm), which facilitates the removal of the tape. This quality makes the tape ideal for glass and other sensitive substrates. BGT-PO180 is a 150µm PO film, with a one-sided 30µm urethane adhesive layer, and backed with a PET liner. This product can be customized according to the customer's needs. 

 

Key Features

  • Back grinding standard compatible
  • Strong adhesion to prevent substrate damage
  • Can be used with uneven surfaces
  • Antistatic
  • High transparency
  • High flexibility
  • High chemical resistance 
  • No residue after removal

Application Ideas

  • Back grinding 
  • Masking
  • Temporary bonding
  • Assembly of delicate components
  • Packaging substrates
  • Glass (e.g. optical applications)
Product Family

BGT-PO180/300

300mm (11.8") wide x 100m (109yd) long

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Acrylic
Appearance
Appearance at room temperature.
Transparent
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
150 µm
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
PET
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
180 μm
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
64748 Oz/in
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
830 lengthwise, 740 crosswise %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
34 lengthwise, 30 crosswise N/cm

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers