BGT-PO130 | Polyolefin Back Grinding Tape

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

BGT-PO130 | Polyolefine Back Grinding Tape

Main features

  • 130 µm film thickness
  • UV Removable acrylic adhesive
  • Back grinding compatible, general purpose

Product Description

LINQTAPE™ BGT-PO130 is a blue translucent polyolefin (PO) tape used in the wafer back grinding process. It is compatible to the BG standard, and is highly accurate. The tape provides an excellent balance of electrical, mechanical, thermal, and chemical properties. PO tapes have the same strong adhesion as a PET tape but are more easily removed from the substrate. This makes it ideal for applications where easy removal without any residue left behind is required. BGT-PO130 is has a low-viscosity adhesive, and is resistant to warpage. 

LINQTAPE™ BGT-PO130 is a 100µm PO film, with a one-sided 30µm acrylic adhesive layer, and backed with a PET liner. This product can be customized according to the customer's needs. 

 

Key Features

  • Back grinding standard compatible
  • Strong adhesion to prevent substrate damage
  • Can be used with uneven surfaces
  • Antistatic
  • High transparency
  • High flexibility
  • High chemical resistance 
  • No residue after removal

Application Ideas

  • Back grinding 
  • Masking
  • Temporary bonding
  • Assembly of delicate components
  • Packaging substrates
  • Glass (e.g. optical applications)
Product Family

BGT-PO130/300

300mm (11.8") wide x 100m (109yd) long

Loading pricing…

Technical Specifications

General Properties
Adhesive Thickness
Adhesive thickness indicates the thickness of an adhesive layer. It refers to the adhesive thickness of a single side so for double sided tapes it always needs to be multiplied.
30 µm
Appearance
Appearance at room temperature.
Blue, Transparent
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
100 µm
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
130 μm
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
4315 Oz/in
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
650 lengthwise, 800 crosswise %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
24 lengthwise, 30 crosswise N/cm

Leading Brands Trust in Our Products and Services