KESTER TSF-6522RH Tacky Soldering Flux

Harmonization Code : 29051200 | Propan-1-ol (propyl alcohol) and propan-2-ol (isopropyl alcohol)

KESTER TSF-6522RH Tacky Soldering Flux

Main features

  • High tack value
  • Long tack life
  • Can reflow in air or nitrogen

Product Description

KESTER TSF-6522RH is a rosin based, no-clean tacky soldering flux formula designed to be compliant with IEC 61249-2-21 definition for halide-free materials. TSF-6522RH is a formula being marketed for customers familiar with Kester's TSF-6522 formula, but now must comply with new halide-free legislation. TSF-6522RH can be used with a doctor blade or a drum fluxer. TSF-6522RH can also be used in dot dispensing for BGA/PGA sites or in a rework application for surface mount packages. TSF-6522RH is classified as ROL0.

Product Key Features

  • High tack values and long tack life
  • ROL0 per J-STD-004B
  • Leaves bright and shiny solder joints
  • Can reflow in air or nitrogen

Applications

  • Soldering in elctronics assembly requiring tacky flux.
Product Family

AP-TSF6522RH/1G0

1g - 30g Syringe - MPN 901003
1. Select Package Type

Loading pricing…

Product availability
Shipping in 3 weeks
Packaging
Unit of measure Syringe
Net weight 0.001 kg
Gross weight 0.01 kg
Dimensions 1 x 1 x 1 cm
TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
285000 mPa.s

Additional Information

Recommended Reflow Profile

Reflow Profile SnAgCu Alloys