KESTER 5252M Cleaner

Harmonization Code : 29051200 | Propan-1-ol (propyl alcohol) and propan-2-ol (isopropyl alcohol)

KESTER 5252M Cleaner

Main features

  • Quickly air dries
  • Halogen-free formulation
  • Non-ionic

Product Description

KESTER 5252M Cleaner is a halogen-free, organic solvent designed for high-performance cleaning in electronics manufacturing and assembly. Environmentally friendly and non-ozone depleting, 5252M offers a safe and effective alternative to traditional chlorinated solvents, especially in applications requiring fast air-drying.

Product Key Features

  • Non-ozone depleting
  • Halogen-free formulation
  • Fast air-drying for time-sensitive cleaning tasks
  • Non-ionic and relatively non-toxic with a mild odor

Applications

Product Family

AP-5252M/1L

1L - 20L Container - MPN 6600045252
1. Select Package Type

Loading pricing…

Product availability
Shipping in 3 weeks
Packaging
Unit of measure Can
Net weight 0.9 kg
Gross weight 1 kg
Dimensions 12 x 12 x 12 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
solubility
100 Min
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.845
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
82 °C
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
16 °C

Additional Information

Application

Usage Instructions

  • 5252M may be used at ambient temperature with ultrasonics, stencil spray equipment, immersion agitation, or manual application.
  • When the residue has completely dissolved and is no longer visible, rinse off the residual solution with more solvent.
  • The goal is not only to dissolve the residue but also to remove it after dissolution.

Drying and Rinsing

  • 5252M dries fast and usually does not require a water rinse.
  • After cleaning, stencils or electronic assemblies should be dried by evaporation or solvent displacement with forced air.
  • For additional cleanliness, a secondary 5252M rinse may be used.

Maintenance

  • The bath life of the cleaner solvent depends on cleanliness requirements.
  • Replace the solvent at regular intervals to avoid contamination.

Leading Brands Trust in Our Products and Services