JNC PI-6302-004 | Insulating Polyimide Ink

Harmonization Code : 3908900090 | Polyamides in Primary form

JNC PI-6302-004 | Insulating Polyimide Ink JNC PI-6302-004 | Insulating Polyimide Ink

Main features

  • Thermal Curable
  • Low Temperature Curing
  • High Heat Resistance

Product Description

PI-6302-004 is a low-temperature cured insulating polyimide ink specially designed to meet the demands of high thermal applications, which provide solution for heat resistance and insulation applications.

PI-6673-004 is engineered to be a thermally curable polyimide ink with remarkable insulating properties making it ideal choice for electrical isolation and heat management applications. Its polyimide-based chemistry brings forth the balance between flexibility and resilience. PI-6673-004 features a residual stress of 32 MPa and a coefficient of thermal expansion (CTE) of 65 ppm/K, ensuring compatibility with various materials and minimizing the risk of performance-altering mismatches. Moreover, with a breakdown voltage of 100 V/um and a dielectric constant of 2.8 @ 1 kHz, ensuring stable electrical isolation and signal integrity for your components.

 

Industry Applications:

Electronics Manufacturing | Consumer Electronics | Sensors and IoT Devices

 

Cure condition

  • 230⁰C in 30 min
Product Family

PI-6302-004/1K

1 kg bottle
1. Select Package Type
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Bottle
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 12 x 12 x 20 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Process Method
Inkjet
Solids
25 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
255 °C
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
100 V/um V
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
10000000000000000 Ohms⋅cm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
3 %
Chemical Properties
Water Absorption
1.0 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
6 mPa.s

Additional Information

Properties PI-6302-004
Solids content (wt. %) 25
Viscosity (mPa's) @25℃ 6
Surface tension (mN/m) @23℃ 27
Printing methods Inkjet
Curing 230℃
30min
Post-curing -
Volume resistivity (Ω*cm) 1E+16
Breakdown voltage (V/um) 100
Dielectric constant (1kHz) @1V 3.5
Tensile modulus (MPa) 780
Elongation (%) 3
Residual stress (MPa) 32
5% weight loss temp (℃) 390
CTE ( 65
Tg (℃) 255
Water absorbance (%) @23℃ 1.0

Leading Brands Trust in Our Products and Services