Product Description

PA-1510-003 is a UV-curable, solvent-free polyacrylate process material with its advanced polyacrylate technology. The material has the properties that provides heat, insulation, impact resistance which can offer temporary protection for any critical components midway to the assembly line process.

PA-1510-003 rapidly cures under UV light, exhibits exceptional filling property wherein its low viscosity allows precise pattern printing application and UV pinning abilities. Boasting water repelling properties this ink confidently resists moisture-induced vulnerabilities, ensuring consistent performance in humid conditions.

Industry Applications:

Microelectronics Mechanical Systems (MEMS) | Assembly Line Component Protection

(Product is EA)
Etching test PA-1510-003

Product Family

PA-1510-003/1K

1kg bottle
1. Select Package Type
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Bottle
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 9 x 9 x 22 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
100 %
solubility
120 Min
Surface Tension
37 mN/m
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
124 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
5.4 mPa.s

Additional Information

Removal process

Etching test with mixture of phosphoric and hydrofluoric acid

Recommended Cleaner usage: 3 times the ink volume