JNC PA-1210-035 | Insulating Polyacrylate Ink

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

JNC PA-1210-035 | Insulating Polyacrylate Ink JNC PA-1210-035 | Insulating Polyacrylate Ink JNC PA-1210-035 | Insulating Polyacrylate Ink JNC PA-1210-035 | Insulating Polyacrylate Ink JNC PA-1210-035 | Insulating Polyacrylate Ink JNC PA-1210-035 | Insulating Polyacrylate Ink JNC PA-1210-035 | Insulating Polyacrylate Ink

Main features

  • UV Curable/ Solvent free
  • High Insulation reliability for thin film devices
  • Optical Devices

Product Description

PA-1210-035 is a UV-curable, solvent-free polyacrylate insulating ink. With its advanced polyacrylate technology, this ink strikes a perfect balance between flexibility and durability. Components coated with PA-1210-035 gain structural integrity capable of withstanding both mechanical stress and temperature fluctuations.

PA-1210-035 rapidly cures under UV light, creating a high-performance insulating layer that not only ensures reliable results but also speeds up your production process. Boasting an ultra-low water absorbance of less than 0.1%, this ink confidently resists moisture-induced vulnerabilities, ensuring consistent performance in humid conditions.

Industry Applications:

Thin Film Electronics | Microfabrication | Optical Devices

Product Family

PA-1210-035/1K

1kg bottle
1. Select Package Type
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Bottle
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 12 x 12 x 20 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Process Method
Inkjet
Solids
100 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
126 °C
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
100 V
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
60000000000000000 Ohms⋅cm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
3 %
Chemical Properties
Water Absorption
0.1 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
35 mPa.s

Additional Information

Properties PA-1210-035
Solids content (wt. %) 100
Viscosity (mPa's) @25℃ 36
Surface tension (mN/m) @23℃ 31
Printing methods Inkjet
Curing 2,000mJ/cm2
 @ 365nm
Post-curing 175℃
60min
Volume resistivity (Ω*cm) 6E+16
Breakdown voltage (V/um) 100
Dielectric constant (1kHz) @1V 3.1
Tensile modulus (MPa) 1400
Elongation (%) 3
Residual stress (MPa) 19
5% weight loss temp (℃) 292
CTE ( 76
Tg (℃) 126
Water absorbance (%) @23℃ <0.1

 

Recommended Cleaner usage: 3 times the ink volume